| 超薄金属膜的电导特性 |
| 范平 |
| 深圳大学理学院;深圳 518060 |
|
引用本文:
范平 . 超薄金属膜的电导特性[J]. 金属学报, 1999, 35(3): 261-264 .
[1] Tang Z L, Huang R F, Wen L S. Acta Metall Sin, 1996; 32:308(唐兆麟,黄荣芳,闻立时.金属学报,1996;32:308) [2] Fuchs K. Proc Cambridge Philos Soc, 1938; 34: 100 [3] Sondheimer E H. Adv Phys, 1952; 1: 1 [4] Mayadas A F, Shatzkes M. Phys Rav, 1970; B1: 1382 [5] Sheng L, Xing D Y, Wang Z D. Phys Red, 1995; B51: 7325 [6] Dong Z C, Sheng L, Xing D Y, Dong J M. Acta Phys Sin,1997: 46: 568(董正超,盛利,邢定玉,董锦明.物理学报, 1997; 46: 568) [7] Wang L H, Huang Y T, Zheng H T. Thin Film Technology.Beijing: Tsinghua University Press, 1991: 70(王力衡,黄运添,郑海涛.薄膜技术.北京:清华大学出版社,1991:70) [8] Hoffmann H. Adv Solid State Phys, 1982; 22: 261G |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|