| 半固态AlSi7Mg合金二次加热工艺与组织转变机制 |
| 张奎 张永忠 |
| 北京有色金属研究总院 北京 100088 |
|
引用本文:
张奎; 张永忠 . 半固态AlSi7Mg合金二次加热工艺与组织转变机制[J]. 金属学报, 1999, 35(2): 127-130 .
[1] Nussbaum A I. Light Met Age, 1996; 54: (5/6):6 [2] Kirkwood D H. Inter Mater Rev, 1994; 39(5): 173 [3] Brown S B, Flemings. Adv Mater Proc, 1993; 143(1): 36 [4] Loue W R, Suery M. Mater Sci Eng, 1995, A203: 1 [5] Flemings M C. Metall Trans , 1991, 22B(6). 269 [6] Zhang K, Liu G J , Lu J N, Zhang Y Z, Fan J Z, Xu J, ZhangS M, Shi L K. Chin J Rare Met, 1998, 22(Suppl): 330(张奎,刘国钧,吕晋宁,张永忠,樊建中,徐骏,张少明,石力开.稀有金属, 1998; 22(增刊): 330) |
|