| 测定高强钢高速冲击动态断裂韧度K_(1d)的新装置及方法 |
| 李强;赖祖涵;马常祥 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳;110015;中国科学院国际材料物理中心;沈阳;110015;东北大学理学院;沈阳;110006 |
|
| A NEW ASSEMBLY AND EVALUATION OF DYNAMIC FRACTURE TOUGHNESS K_(1d) OF HIGH STRENGTH STEEL AT HIGH VELOCITY IMPACT |
| LI Qiang(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)LAI Zuhan(International Centre for Material Physics; The Chinese Academy of Sciences; Shenyang 110015)MA Changxiang(College of Sciences; Northeastern University; Shenyang 110006)Correspondent: LI Qiang; Tel: (024)23843531-55659; Fax: (024)3891320; E-mail: qli imr ac.cn |
引用本文:
李强;赖祖涵;马常祥. 测定高强钢高速冲击动态断裂韧度K_(1d)的新装置及方法[J]. 金属学报, 1998, 34(8): 852-857.
,
,
.
A NEW ASSEMBLY AND EVALUATION OF DYNAMIC FRACTURE TOUGHNESS K_(1d) OF HIGH STRENGTH STEEL AT HIGH VELOCITY IMPACT[J]. Acta Metall Sin, 1998, 34(8): 852-857.
1 Donald A. Dynamic Fracture Testing, Metals Handbook Vo1.8, New York: ASM, 1985: 259 2 Kobayashi T. Eng Fract Mech, 1984; 19: 49 3 Kobayashi T. Eng Fract Mech 1984; 19: 67 4 Kishimoto K, Aoki S, Sakata M. Eng Fract Mech 1980; 13: 501 5 Nash G E. Int J Fract Mech, 1969; 15: 269 6 Lee Y, Prakash V. Metoll Mater Trans, 1995; 26A: 2527 7 Tang C A, Xu X H. Eny Fract Mech 1990; 35(4/5): 783 8 Kalthoff J F. Int J Fract, 1985; 27: 277 9 Martin E, Mack T, Quenisset J M. Eng Fract Mech 1986; 24: 821 10 Liu Y N, Zhu J H, Zhou H J. Eng Fract Mech 1991; 39: 955 |
|