| Ti吸附Hg后位错发射及微裂纹形核的TEM原位研究 |
| 宿彦京;吕宏;王燕斌;褚武扬 |
| 北京科技大学材料物理系;北京;100083;北京科技大学材料物理系;北京;100083;北京科技大学材料物理系;北京;100083;北京科技大学材料物理系;北京;100083 |
|
| IN SITU TEM STUDY OF DISLOCATION EMISSION AND MICROCRACK NUCLEATION FOR α-Ti AFTER ADSORBING Hg |
| SU Yanjing; LU Hong; WANG Yanbin; CHU Wuyang (Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083) |
引用本文:
宿彦京;吕宏;王燕斌;褚武扬. Ti吸附Hg后位错发射及微裂纹形核的TEM原位研究[J]. 金属学报, 1998, 34(4): 337-344.
,
,
,
.
IN SITU TEM STUDY OF DISLOCATION EMISSION AND MICROCRACK NUCLEATION FOR α-Ti AFTER ADSORBING Hg[J]. Acta Metall Sin, 1998, 34(4): 337-344.
1 Nicholas M G, Old C F.J Mater Sci, 1979; 14: 1 2 Kamdar M H. Progr, Mate, Sci, 1973; 15: 189 3 Kelley M J, Stoloff N S. Metall Trans, 1975; 6A: 159 4Lynch S P. Acta Metall, 1988; 36: 2639 5Chen Q Z, Chu W Y; Hsiao C M. Acta Metall Mater, 1995; 43: 4371 6 张 跃,王燕斌,褚武扬,肖纪美.中国科学,1994;A24:551Zhang Yue,Wang Yanbin,Chu Wuyang,Xiao Jimei. Sci Chin,1994; A24:551) 7高克玮,陈奇志,褚武扬,肖纪美.中国科学, 1994; A24: 993 8 (Gao Kewei,Chen Qizhi,Chu Wuyang,Xiao Jimei.Sci Chin, 1994; A24:993)8 谷飙,高克玮,黄一中,褚武扬中国科学,1996;E26:4819(Gu Biao,Gao Kewei, Huang Yizhong,Chu Wuyang. Sci Chin, 1996; E26:481)9宿彦京,王燕斌,褚武扬科学通报,19972 42:1 (Su Yanjing,Wang Yanbin,Chu Wuyang Chin Sci Bull, 1997; 42:1) 10Worner N W. Bull Inst Met, 1954; 12(2): 141 11Chen C M, Kirkpatrick H B Corrosion, 1970 ;26: 559 12 Ohr S M. Mater Sci Eng, 1985; 72: 1 13Zhu T, Yang W, Guo T Acta Mater, 1996 44: 3049 14 Cherepanov G P.Mechanics of Brittle Fracture. New York:McGraw-Hill Inc,1979:29 15Kargol J A, Albrighy D L. Metall Trans, 1977; 8A: 27 16Dewald D K, Lee T C, Robertson I M, Birnbaum H K Scr Metall, 1989; 23: 1307 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|