| 合金元素对Ni_3Al合金抗汽蚀性能的影响 |
| 叶武俊;冯涤;陈蓓京;骆合力 |
| 北京钢铁研究总院;北京;100081;北京钢铁研究总院;北京;100081;北京钢铁研究总院;北京;100081;北京钢铁研究总院;北京;100081 |
|
| EFFECT OF METALLURGICAL FACTORS ON THE RESISTANCE OF CAVITATION EROSION OF Ni_3Al BASED ALLOYS |
| YE Wujun;FENG Di;CHEN Beijing;LUO Heli (Central Iron and Steel Research institute; BeiJing 100081) |
引用本文:
叶武俊;冯涤;陈蓓京;骆合力. 合金元素对Ni_3Al合金抗汽蚀性能的影响[J]. 金属学报, 1998, 34(11): 1163-1166.
,
,
,
.
EFFECT OF METALLURGICAL FACTORS ON THE RESISTANCE OF CAVITATION EROSION OF Ni_3Al BASED ALLOYS[J]. Acta Metall Sin, 1998, 34(11): 1163-1166.