| 板坯中间包钢水流动的热态水模 |
| 王建军;戴朝珊;周俐;张玉柱;李正邦;肖泽强 |
| 华东冶金学院;马鞍山;243002;华东冶金学院;马鞍山;243002;华东冶金学院;马鞍山;243002;邯郸钢铁公司;邯郸;056000;冶金工业部钢铁研究总院;北京;100081;东北大学;沈阳;110006 |
|
| FLOWING SIMULATION OF MOLTEN STEEL IN SLAB TUNDISH BY HOT WATER MODEL |
| WANG Jianjun;DAI Chaoshan;ZHOU Li(East China Institute of Metallurgy;Ma'anshan 243002); ZHANG Yuzhu (Handan Iron and Steel Co.; Handan 056000);LI Zhenghang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081); XIAO Zeqiang (Northeastern University; Shenyang 110006) |
引用本文:
王建军;戴朝珊;周俐;张玉柱;李正邦;肖泽强. 板坯中间包钢水流动的热态水模[J]. 金属学报, 1997, 33(5): 509-514.
,
,
,
,
,
.
FLOWING SIMULATION OF MOLTEN STEEL IN SLAB TUNDISH BY HOT WATER MODEL[J]. Acta Metall Sin, 1997, 33(5): 509-514.