| 准分子激光预处理对硬质合金表面沉积金刚石薄膜结合强度的影响 |
| 李成明;王建明;徐重;吕反修;王建军 |
| 太原工业大学表面工程研究所;北京科技大学 |
|
| EFFECT OF EXCIMER LASER PRETREATMENT ON DIAMOND FILM DEPOSITED ON HARD ALLOY SUBSTRATE |
| LI Chengming; WANG Jianming; XU Zhong (Taijuan University of Technology; Taiyuan 030024)LU Fanxiu; WANG Jianjun (University of Science and Technology Beijing; Beijing 100083) |
引用本文:
李成明;王建明;徐重;吕反修;王建军. 准分子激光预处理对硬质合金表面沉积金刚石薄膜结合强度的影响[J]. 金属学报, 1996, 32(9): 966-970.
,
,
,
,
.
EFFECT OF EXCIMER LASER PRETREATMENT ON DIAMOND FILM DEPOSITED ON HARD ALLOY SUBSTRATE[J]. Acta Metall Sin, 1996, 32(9): 966-970.
| 1MurakawaM.SurCoatTechnol,1988;36:3032KikuchiW.JPPat.63-53268,19883SaitoY,SatoK,MatudaS,KoinumaH.JMatSci.1991;26:29374SaijoK,YagiM,ShibukiK,SadahiroT.JPPat,03-20467,19915MurakawaM,TakeuchiS.ThinSolidFilms,1989;181:1436KawaiC.JPPat,04-2401,1992 |
|