| 5454铝镁合金与工业纯铝管在碳化液中形成的表面膜研究 |
| 方耀华;张明杰;孙玉珍;王文皓 |
| 南京化工大学;中国科学院金属研究所 |
|
| RESEARCH ON SURFACE FILMS FORMED BY 5454 Al-Mg ALLOY TUBE AND PURE ALUMINIUM TUBE IN CARBONATED SOLUTION |
| FANG Yaohua; ZHANG Mingjie(Nanjing University of Chemical Technology; Nan jing 210009);SUN Yuzhen; WANG Wenhao (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuseript received 1995-12-15) |
引用本文:
方耀华;张明杰;孙玉珍;王文皓. 5454铝镁合金与工业纯铝管在碳化液中形成的表面膜研究[J]. 金属学报, 1996, 32(7): 763-768.
,
,
,
.
RESEARCH ON SURFACE FILMS FORMED BY 5454 Al-Mg ALLOY TUBE AND PURE ALUMINIUM TUBE IN CARBONATED SOLUTION[J]. Acta Metall Sin, 1996, 32(7): 763-768.