| 凝固速率对定向凝固合金DZ22枝晶臂间距和枝晶偏析的影响 |
| 刘忠元;李建国;傅恒志 |
| 西北工业大学 |
|
| DENDRITIC ARM SPACING AND MICROSEGREGATION OF DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ22 AT V ARIOUS SOLIDIFICATION RATES |
| LIU Zhongyuan;LI fianguo;FU Hengzhi(Faculty No;403;NorthwesternPolytechnical University;Hi'an 710072)(Manuscipt received 1994-11-21) |
引用本文:
刘忠元;李建国;傅恒志. 凝固速率对定向凝固合金DZ22枝晶臂间距和枝晶偏析的影响[J]. 金属学报, 1995, 31(7): 329-332.
,
,
.
DENDRITIC ARM SPACING AND MICROSEGREGATION OF DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ22 AT V ARIOUS SOLIDIFICATION RATES[J]. Acta Metall Sin, 1995, 31(7): 329-332.
| 1李建国,储双杰,刘忠元,史正兴,傅恒志,材料工程,1991;1:42-442CHUShuangjie,LIJianguo,LIUZhongyuan,SHIZhengxing,FUHengzhi.MetallTrans,1994;25A:637-6423 刘忠元,杨爱民,李建国,史正兴,傅恒志.材料科学进展,1992;6(6):481-4864 王罗宝,陈荣章,王玉屏.铸造高温合金论文集,1986:35-405毛协民,傅恒志.周尧和.西北工业大学学报,1985;3(1):11-20 |
|