Please wait a minute...
金属学报  1995, Vol. 31 Issue (23): 499-504    
  论文 本期目录 | 过刊浏览 |
热固树脂-K08Al钢层状复合板的成形性及减振性
程娴;英哲;陈礼清;张磊;刘文忠
中国科学院金属研究所;长春第一汽车制造厂;中国科学院长春应用化学研究所
FORMING AND VIBRATION-DAMPING BEHAVIOUR OF LAMINATED SHEET STEEL WITH THERMOSET RESIN
CHENG Xian;YING Zhe;CHEN Liqing(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015);ZHANG Lei(Changchun No.1 Automobile Works;Changchun 130011);LIU Wenzhong(Institute of Changchun Applied Chemistry;Chinese Academy of Sciences;Changchun 130022)(Manuscript received 1995-04-07;in revised form 1995-05-16)
引用本文:

程娴;英哲;陈礼清;张磊;刘文忠. 热固树脂-K08Al钢层状复合板的成形性及减振性[J]. 金属学报, 1995, 31(23): 499-504.
, , , , . FORMING AND VIBRATION-DAMPING BEHAVIOUR OF LAMINATED SHEET STEEL WITH THERMOSET RESIN[J]. Acta Metall Sin, 1995, 31(23): 499-504.

全文: PDF(447 KB)  
摘要: 研究了由几种不同基团比和的热固性树脂与K08Al薄钢板组成的层状复合板的力学性能、成形性及减振性。结果表明,仅用应变硬化指数n值和塑性应变比r值不足以充分评定复合钢板的成形性。在复合钢板设计时应考虑到表皮钢板应具有良好的成形性,其间的粘接强度应超过13MPa复会钢板的使用温度在其夹层材料的玻璃化温度约±15℃内可获得最佳减振性能。
关键词 : 层状复合钢板,  热固树脂,  成形性,  减振性    
Abstract:The laminated damping steels composed of K08Al deep-drawing steel and thermoset resin with several different sum of mole ratio are prepared to study the mechanical properties,forming and vibration-damping behaviour.The results show that the n and r values are insufficient to evaluate the formability of the laminated damping steels.In design of the laminated damping steels the skin sheet steel with excellent formability should be selected and the steel-resin-steel sheets must have 13 MPa shear bonding strength or more.In order to obtain the optimum damping effect,the working temperature of the laminated damping sheets should be within±15℃ of the vitrification point of the resin.
Key words: laminated damping sheet steel    thermoset resin    formability    vibration-damping behaviour
    
基金资助:国家自然科学基金
1DicelloJA.SAEPaper,No.800078,19802MckennaLW,WohlMH,WoodbreyJC.SAEPaper,No.800079,19803MillerWK.SAEPaper,No.800077,19804HashimotoK,OhwucT,TakitaM.Proc15thIntDeepDrawingResearchGroupBiennialCongress.Dearborn,Michigan,USA,1988:2835ChengX,ZhangL,LiuW.Proc16thIntDeepDrawingResearchGroupBiennialCogress,Borlange,Sweden,1990:2156ChenH,FoggB.SheetMetInd,1982;(6):5127ChengX,ZhangL,LiuW.Proc1991IntDeepDrawingResearchGroupWorkingGroupsMeeting,Pisa,Italy,1991|
[1] 娄峰, 刘轲, 刘金学, 董含武, 李淑波, 杜文博. 轧制态Mg-xZn-0.5Er合金板材组织及室温成形性能[J]. 金属学报, 2023, 59(11): 1439-1447.
[2] 潘复生, 蒋斌. 镁合金塑性加工技术发展及应用[J]. 金属学报, 2021, 57(11): 1362-1379.
[3] 刘后龙,马明玉,刘玲玲,魏亮亮,陈礼清. 热轧板退火工艺对19Cr2Mo1W铁素体不锈钢织构与成形性能的影响[J]. 金属学报, 2019, 55(5): 566-574.
[4] 陈懿, 郭明星, 易龙, 袁波, 李高洁, 庄林忠, 张济山. 新型Al-Mg-Si-Cu-Zn合金板材组织、织构和性能的优化调控[J]. 金属学报, 2017, 53(8): 907-917.
[5] 惠亚军, 潘辉, 刘锟, 李文远, 于洋, 陈斌, 崔阳. 600 MPa级Nb-Ti微合金化高成形性元宝梁用钢的强化机制[J]. 金属学报, 2017, 53(8): 937-946.
[6] 张艳,郭明星,邢辉,王斐,汪小锋,张济山,庄林忠. 不同热加工工艺对Al-Mg-Si-Cu合金板材力学性能和组织的影响*[J]. 金属学报, 2015, 51(12): 1425-1434.
[7] 王成国;孙希泰;彭其凤;朱静;蔡其巩. 层压减振复合钢板减振性能的温度依存性[J]. 金属学报, 1995, 31(22): 451-454.
[8] 王春荣;宋海龙;曲力;曹淑芝. 超塑气胀构件可成形性判据的数学模型[J]. 金属学报, 1989, 25(6): 152-155.