| 非晶态Fe-B-Si合金的退火脆化 |
| 车晓舟;胡赓祥;曹兴国;戴礼智 |
| 上海交通大学;洛阳工学院;冶金工业部钢铁研究总院 |
|
| ANNEALING EMBRITTLEMENT OF AMORPHOUS Fe-B-Si ALLOYS |
| CHE Hiaozhou; HU Gengxiang(Shanghai Jiaotong University); CAO Hingguo(Luoyang Institute of Technology); DAI Lizhi(Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
引用本文:
车晓舟;胡赓祥;曹兴国;戴礼智. 非晶态Fe-B-Si合金的退火脆化[J]. 金属学报, 1994, 30(24): 532-536.
,
,
,
.
ANNEALING EMBRITTLEMENT OF AMORPHOUS Fe-B-Si ALLOYS[J]. Acta Metall Sin, 1994, 30(24): 532-536.
| 1张传历.国外金属材料,1982;11:392LuborskyFE,WalterJL,JApplPhys,1976;47:36483车晓舟,曹兴国,戴礼智.机械工程材料,1993;17(4):174YamasakiT,TakahashiM,OginoY,In:SteebS,WarlimontHeds.,RapidlyQuenchedMetals,Vol.II,ElsevierSciencePublishersB.V.,1984:13815WangJT,PangDX,SongQH,DingBZ.MaterSciEng,1988;98:5356ChiGC,ChenHS,MillerCE.JApplPhys,1978;49:1715f |
|