| 球状生长与单向凝固的溶质分布对比 |
| 吴锵;刘驰 |
| 南京理工大学;东南大学 |
|
| COMPARISON OF SOLUTE DISTRIBUTION BETWEEN SPHERICAL GROWTH AND DIRECTIONAL SOLIDIFICATION |
| WU Qiang;LIU Chi Nanjing University of Science and Technology Southeast University |
引用本文:
吴锵;刘驰. 球状生长与单向凝固的溶质分布对比[J]. 金属学报, 1993, 29(9): 42-46.
,
.
COMPARISON OF SOLUTE DISTRIBUTION BETWEEN SPHERICAL GROWTH AND DIRECTIONAL SOLIDIFICATION[J]. Acta Metall Sin, 1993, 29(9): 42-46.
1 《数学手册》编写组.数学手册.北京:高等教育出版社,1983:216 2 Kurz W,Fisher D J著;毛协民,包冠乾译.凝固原理.西安:西北工业大学出版社,1987:159 |
|