APPLICATION OF d-ELECTRON ALLOY DESIGN THEORY TO DEVELOPMENT OF HOT CORROSION RESISTANT Ni-BASE SINGLE CRYSTAL SUPERALLOYS——Ⅰ Characterization of Phase Stability |
ZHANG Jishan;CUI Hua;HU Zhuangqi;MURATA Y;MORINAGA M;YUAA WA N Institute of Metal Research; Academia Sinica; Shenyang Toyohashi University of Technology; Japanassociate professor;Institute of Metal Research;Academia Sinica;Shenyang 110015 |
引用本文:
张济山;崔华;胡壮麒;村田纯教;森永正彦;汤川夏夫. 应用d—电子合金设计理论发展新型抗热腐蚀单晶镍基高温合金 Ⅰ.相稳定性临界条件的确定[J]. 金属学报, 1993, 29(7): 5-12.
,
,
,
,
,
.
APPLICATION OF d-ELECTRON ALLOY DESIGN THEORY TO DEVELOPMENT OF HOT CORROSION RESISTANT Ni-BASE SINGLE CRYSTAL SUPERALLOYS——Ⅰ Characterization of Phase Stability[J]. Acta Metall Sin, 1993, 29(7): 5-12.
1 Cetel A D, Duhl D N, Proc of Inter Symp on Superalloys, Superalloys 1988. ed. Duhl D N, Maurer G, Antolovic S h, Lund C and Reichmall S, Seven Springs, Sept., 1988, TMS, W arrendale, 1988, 235. 2 Harris K, Erickson G L, Scher R E, Proc of Conf on High Temperature Alloys for Gas Turbines and Other Applications, ed. W. Betzetal, Oct., 1986, D. Reidel Publishing Compony, Dordrecht, Holland, 1986, 709. 3 Ford D A, Arthery P R, Proc of Inter Symp on Superalloys, Superalloys 1984, ed. Gell N, et al., Seven Springs, 1984, TMS, Warrendale, 1984, 115. 4 Yamagata T, Harata H. Nagazawa A, Yamazaki M, Naka zawa Y G, ibid, 157 5 Yukawa N, Morinaga M, Murata Y, Ezaki H, Inoue S, Proc of Symp on Superalloys, Superalloys 1988, ed. Duhl D N et al, Seven Springs, 1988, TMS, Warrendale, 1988, 255. 6 Morinaga M, Yukawa N, Adachi H, J Phy Soci Jpn., 53 (1984) 653. 7 Morinaga M, Yukawa N, Ezaki H, Phil Mag A, 51 (1985) 247 8 Morinaga M, Yukawa N, Ezaki H, Phil Mag A, 51 (1985) 257. 9 Yukawa N, Morinaga M, Ezaki H, Murata Y, Proc of Conf on High Temperature Alloys of Gas Turbines and Other Applications ed. Betz et al, Oct., 1986, D. Reidel Publishing Compony, Dordrecht, Holland, 1986, 935. 10 Beltran A M, Show D A, Superalloys. ed. Simsand C T, Hagel W C, A Wiley-Interscience Publication, 1972, 317. 11 LomBardi G, For Better Thermal Analysis, 2nd ed., (1980) 24 |
|