| 机械合金化扩展Fe—Cu系固溶范围 |
| 杨元政;马学鸣;董远达 |
| 中国科学院固体物理研究所;中国科学院固体物理研究所;中国科学院固体物理研究所;研究员;合肥(230031) |
|
| EXTENSION OF SOLID SOLUBILITY BY MECHANICAL ALLOYING IN Fe-Cu SYSTEM |
| YANG Yuanzheng; MA Xueming; DONG Yuanda (Institute of Solid State Physics; Academia sinica; Hefei) |
引用本文:
杨元政;马学鸣;董远达. 机械合金化扩展Fe—Cu系固溶范围[J]. 金属学报, 1992, 28(9): 25-29.
,
,
.
EXTENSION OF SOLID SOLUBILITY BY MECHANICAL ALLOYING IN Fe-Cu SYSTEM[J]. Acta Metall Sin, 1992, 28(9): 25-29.
1 Steeb S, Warlimont H. Rapidly Quenched Metals. Amstrdam: North-Holland, 1985 2 Kneller E F. J Appl Phys, 1964; 35: 2210 3 Van Mourik P, Mittemeiser E J, De Keijser T H. J Mater Sci, 1983; 18:2706 4 Sumiyama K, Nakamura Y. Phys Status Solidi, 1984; a81:K109 5 Benjamin J S. Metall Trans, 1970; 1: 2943 6 Schultz L. Mater Sci Eng, 1988; 97: 15 7 Eckert J, Schultz L. J Less-Common Met, 1991; 166:293 8 Shingu P H, Ishihara K N, Uenishi K. In: Clauer A H, De Barbadillo J J eds., Solid State Powder Processing, The Minerals Metals and Materials Society, 1990: 20 9 Campbell S J. Clark P E. J Phys F: Metal Phys, 1974; 4:1073 10 Uenishi K, Kobayashi K F, Ishihara K N, Shingu P H, Mater Sci Eng, 1991; A134: 1342 11 Schumacher S, Birringer R, StrauB R, Gleiter H. Acta Metall, 1989; 37: 2485* |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|