| Fe-Ni-C相图的550,450℃等温截面 |
| 龚方岳;GoldsteinJI |
| 天津大学材料系;副教授;天津(300072);美国Lehigh大学 |
|
| 550 AND 450℃ ISOTHERMAL SECTIONS OF Fe-Ni-C PHASE DIAGRAM |
| GONG Fangyue;GOLDSTEIN JI Tianjin University; Lehigh University; Bethlehem; U. S. A. Correspondent associate professor; Department of Materials Science; Tianjin University; Tianjin 300072 |
引用本文:
龚方岳;GoldsteinJI. Fe-Ni-C相图的550,450℃等温截面[J]. 金属学报, 1992, 28(6): 47-51.
,
.
550 AND 450℃ ISOTHERMAL SECTIONS OF Fe-Ni-C PHASE DIAGRAM[J]. Acta Metall Sin, 1992, 28(6): 47-51.
1 Romig A D, Goldstein J I. Metall Trans, 1978; 9A: 1599 2 Bastin G F, Van Loo F J J, Heijiligers H J M. X-Ray Spectros, 1984; 13: 91 3 Porter D A. Easterling K E. Phase Transformations in Metals and Alloys. New York: Van Nostrand reinholod Co. 1981: 280 4 Romig A D Jr., Goldstein J I. Metall Trans, 1980; 11A: 1151 |
|