金属学报  1992, Vol. 28 Issue (6): 52-58    
  论文 本期目录 | 过刊浏览 |
C-Fe-X(X=Mn,Si,Cr,Ni)熔体中组元活度的解析
蒋国昌;张晓兵;徐匡迪
上海工业大学冶金及材料工程系;上海(200072);上海工业大学冶金及材料工程系;上海工业大学冶金及材料工程系
EVALUATION OF COMPONENT ACTIVITY IN C-Fe-X(X=Si; Mn, Cr, Ni) MELTS
JIANG Guochang;ZHANG Xiaobing;XU Kuangdi Shanghai University of Technology Correspondent Department of Metallargy and Materials Engineering; Shanghai University of Technology; Shanghai 200072
引用本文:

蒋国昌;张晓兵;徐匡迪. C-Fe-X(X=Mn,Si,Cr,Ni)熔体中组元活度的解析[J]. 金属学报, 1992, 28(6): 52-58.
, , . EVALUATION OF COMPONENT ACTIVITY IN C-Fe-X(X=Si; Mn, Cr, Ni) MELTS[J]. Acta Metall Sin, 1992, 28(6): 52-58.

全文: PDF(415 KB)  
摘要: 将过剩自由能表达为组元的多项式函数。以该体系液相区边界条条件为基础,用拟合法确定碳偏mole自由能表达式中的参数,然后,用“I—D”法给出组元X的活度系数,此法可以确定各C—Fe—X系整个液相区中任一组元的活度,解析结果与文献上的试验结果吻合得很好。
关键词 组元活度系数C-Fe-Mn系C-Fe-Si系C-Fe-Cr系C-Fe-Ni系    
Abstract:The parameters in the polynomial expression of partial mole free energy of Cwere evaluated by value fitting method on the basis of boundary conditions of liquid domainon the system C-Fe-X(X=Si, Mn, Cr, Ni). Then the activity coefficient of the element Xmaybe calculated with the I-D method. The approach suggested is proved to be useful for theactiveity evaluation of every element in the whole liquid domain of the concerncd 4C-Fe-Xternary systems. The results are found in a good agreement with those of citedprovious literatures.
Key wordscomponent activity coefficient    C-Fe-Mn system    C-Fe-Si system    C-Fe-Cr system    C-Fe-Ni system
收稿日期: 1992-06-18     
1 Pelton A D, Flengas S N. Can J chem, 1969; 47: 2283--2293
2 王之昌.中国科学(A),1986;(8) :862-873
3 王之昌.私人通讯
4 Hultgren R et al. Selected Values of Thermodynamic Properties of Metals and Alloys. New York: Wiley. 1973: 485
5 Kubaschewsk O et al., Metallurgical thermochemistry. 5th ed, Oxford: Pergamon, 1979
6 Elliott J F, Gleiser M, Ramakrishna V. Thermochemistry for Steelmaking. Vol. Ⅱ Thermodynamic and Transport Propertties, London: Addison-Wesley, 1963
7 Darken L S. Trans Metall Soc AIME 1967; 239: 90--96
8 Dresler W. ISM, 1990: 95--99
9 Griffing N R, Forgeng W D, Healy G W. Trans Metall Soc AIME, 1962; 224: 148--158
10 Dresler W. Electr Furace Conf Proc, 1989; 47: 49--55
11 Dresler W. Can Metall Q, 1989; 28: 109--115
12 张晓兵.上海工业大学学报,1990;11;490--496
13 Turkdogan E T. Iron Steel Inst Jpn, 1956; 5: 69--72G
No related articles found!