| SiO_2在铝酸钠溶液中存在状态的研究 |
| 柳妙修;周佩芳;陈念贻;李郁;柯家骏 |
| 中国科学院上海冶金研究所;中国科学院上海冶金研究所;中国科学院上海冶金研究所;研究员;上海(200050);上海科技大学;中国科学院化工冶金研究所 |
|
| ON ANIONIC SPECIES OF SiO_2-CONTAINING SODIUM ALUMINATE SOLUTIONS |
| LIU Miaoxiu;ZHOU Peifang;CHEN Nianyi;LI Yu;KE Jiajun Shanghai Institute of Metallurgy; Academia Sinica Shanghai University of Science and Technology Institute of Chemical Metallurgy; Academia Sinica; Beijing professor |
引用本文:
柳妙修;周佩芳;陈念贻;李郁;柯家骏. SiO_2在铝酸钠溶液中存在状态的研究[J]. 金属学报, 1990, 26(3): 146-149.
,
,
,
,
.
ON ANIONIC SPECIES OF SiO_2-CONTAINING SODIUM ALUMINATE SOLUTIONS[J]. Acta Metall Sin, 1990, 26(3): 146-149.
1 陈念贻.氧化铝生产的物理化学,上海科技出版社,1962:102 2 Guth J L, Caullet P, Jacques P, Wey R. Bull Soc Chim Fr, 1980; (3--4) : I--122 3 #12 4 #12 5 Moolenaar R J, Evans J C, McKeever L D. J Phys Chem, 1970; 74: 3629 6 Marinangeli A, Morelli M A, Simoni R, Bertoluzza A. Canadian Journal of Spectroscopy, 1978; 23: 173 |
|