| 工业纯铜的异步冷轧及再结晶织构研究 |
| 刘燕声;赵骧;梁志德 |
| 东北工学院金属材料系;沈阳110006;东北工学院;东北工学院 |
|
| COLD ROLLING TEXTURE AND RECRYSTALLIZATION TEXTURE OF CROSS SHEAR ROLLED COMMERCIAL COPPER |
| LIU Yansheng;ZHAO Xiong;LIANG Zhide Northeast University of Technology; Shenyang Department of Materials Science and Engineering;Northeast University of Technology;Shenyang 110006 |
引用本文:
刘燕声;赵骧;梁志德. 工业纯铜的异步冷轧及再结晶织构研究[J]. 金属学报, 1990, 26(3): 126-130.
,
,
.
COLD ROLLING TEXTURE AND RECRYSTALLIZATION TEXTURE OF CROSS SHEAR ROLLED COMMERCIAL COPPER[J]. Acta Metall Sin, 1990, 26(3): 126-130.
1 朱泉.钢铁,1980;15:1 2 梁志德,徐家桢,王福.织构材料的三继取向分析术,沈阳:东北工学院出版社,1986:108 3 Taylor G I. J Inst Met. 1938; 62: 307 4 Houtte P V, Aernoudt E. Z Metallk. 1975; 66: 202 5 刘燕声,梁志德.科学通报,1989;6:471] |
|