| 稀土元素在铁液中与碳相互作用的研究 |
| 杜挺;乐可襄 |
| 冶金部钢铁研究总院;冶金部钢铁研究总院 |
|
| INTERACTION BETWEEN RARE EARTH ELEMENTS AND CARBON IN LIQUID IRON |
| by DU Ting; YUE Kexiang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 21 January; 1985; revised manuscript 23 July; 1986) |
引用本文:
杜挺;乐可襄. 稀土元素在铁液中与碳相互作用的研究[J]. 金属学报, 1987, 23(4): 385-388.
,
.
INTERACTION BETWEEN RARE EARTH ELEMENTS AND CARBON IN LIQUID IRON[J]. Acta Metall Sin, 1987, 23(4): 385-388.