| 线型精炼方法中两种函数的比较 |
| 张志焜;崔相旭;王煜明 |
| 吉林大学;吉林大学;吉林大学 |
|
| COMPARISON OF TWO FUNCTIONS FOR X-RAY DIFFRACTION FITTING |
| by ZHANG Zhikun;CUI Xiangxu; WANG Yuming (Jilin University; changchun) (Manuscript received 11 May; 1985; revised manuscript 28 April; 1986) |
引用本文:
张志焜;崔相旭;王煜明. 线型精炼方法中两种函数的比较[J]. 金属学报, 1987, 23(4): 389-392.
,
,
.
COMPARISON OF TWO FUNCTIONS FOR X-RAY DIFFRACTION FITTING[J]. Acta Metall Sin, 1987, 23(4): 389-392.
1 Keijser Th H De, Mittemeijer E J, Rozendaal H C F. J Appl Crystallogr, 1983; 16: 309-316 2 Keijser Th H De, Langford J I, Mittemeijer E J, Vogels A B P. J Appl Crystallogr 1982; 15:308-314 3 Alexander L, Klug H P. Anal Chem, 1948 20:886-889 4 Naidu S V N, Houska C R. J Appl Crystallogr, 1980; 15:190-19 |
|