| NaF-CaCl_2-LiCl系熔盐相图的研究 |
| 阎立诚;杨金秀;朱鹦鹦 |
| 上海科技大学;上海科技大学;上海科技大学 |
|
| PHASE DIAGRAM OF NaF-CaCl_2 -LiCl SYSTEM |
| by YAN Licheng; YANG Jinxiu; ZHU Yingying (Shanghai University of Science and Technology) (Manuscript received 6 January; 1986; revised manuscript 21 July; 1986) |
引用本文:
阎立诚;杨金秀;朱鹦鹦. NaF-CaCl_2-LiCl系熔盐相图的研究[J]. 金属学报, 1987, 23(4): 382-384.
,
,
.
PHASE DIAGRAM OF NaF-CaCl_2 -LiCl SYSTEM[J]. Acta Metall Sin, 1987, 23(4): 382-384.
1 阎立诚,朱鸚鹦,陈念贻.高等学校化学学报,1984;6(5) :755 2 Grube G, Rucel W.JCP Reference Data, 1975; 4(4) : 959 3 #12 4 #12 5 #12 6 #12 7 陈念贻,张桂成,金属学报,1961;7:11 |
|