| 电子束相变硬化处理表面温度场的数值计算 |
| 赵海鸥;冯燕武;唐传芳;朱沅浦 |
| 机械部北京机电研究所;机械部北京机电研究所;机械部北京机电研究所;机械部北京机电研究所 |
|
| NUMERICAL CALCULATION OF TEMPERATURE DISTRIBUTION DURING ELECTRON BEAM TRANSFORMATION HARDENING |
| by ZHAO Hai'ou; FENG Yanwu; TANG Chuanfang; ZHU Yuanpu (Beijing Research Institute of Mechanical and Electrical Technology; Ministry of Machine Building Industry) (Manuscript received 10 January; 1986; revised manuscript 9 April; 1986) |
引用本文:
赵海鸥;冯燕武;唐传芳;朱沅浦. 电子束相变硬化处理表面温度场的数值计算[J]. 金属学报, 1987, 23(4): 368-378.
,
,
,
.
NUMERICAL CALCULATION OF TEMPERATURE DISTRIBUTION DURING ELECTRON BEAM TRANSFORMATION HARDENING[J]. Acta Metall Sin, 1987, 23(4): 368-378.
1 Kou S, Sun D K, Le Y P. Metall Trans, 1983; 14A: 643. 2 Mawella K J A. Met Sci, 1984; 18:549 3 Mazumder J, Steen W M. J Appl Phys, 1980; 51:941 4 川寄一博,高岡憲久,山崎隆雄,尾崎良二.热处理,1980;20(6) :281 5 刘云旭主编.金属热处理原理,机械工业出版社,1981:17,191 6 横田清義,铁钢急速加热变态研究,中島宏,東京,1971;10 1971 7 房为捷,于志勤.金属热处理,1982;(6) :1 |
|