| 超塑气胀构件的可成形性判据 |
| 王春荣;曹淑芝 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| CRITERIA OF FORMABILITY OF COMPONENTS BY SUPERPLASTIC AIR BULGE |
| by WANG Chunrong; CAO Shuzhi (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 15 April; 1986; revised manuscript 1 July; 1986) |
引用本文:
王春荣;曹淑芝. 超塑气胀构件的可成形性判据[J]. 金属学报, 1987, 23(4): 363-367.
,
.
CRITERIA OF FORMABILITY OF COMPONENTS BY SUPERPLASTIC AIR BULGE[J]. Acta Metall Sin, 1987, 23(4): 363-367.