4D打印316L/Invar36异质金属结构的界面特征及其热激励变形行为

李建卫1,2 杨海欧1,2 吴昱涵1,2 李俊杰2 王志军2 王锦程2

1 西北工业大学 深圳研究院  深圳 518057

2 西北工业大学 凝固技术国家重点实验室  西安 710072

Interface Characteristics and Thermal Deformation Behavior of 4D Printed 316L/Invar36 Heterogeneous Metal Structures 

LI Jianwei 1, YANG Haiou 1,2, WU Yuhan 1, LI Junjie 1, WANG Zhijun 1, WANG Jincheng 1

1 Shenzhen Research Institute, Northwestern Polytechnical University, Shenzhen 518057, China

2 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072, China

引用本文:

李建卫 杨海欧 吴昱涵 李俊杰 王志军 王锦程. 4D打印316L/Invar36异质金属结构的界面特征及其热激励变形行为[J]. 金属学报, DOI: 10.11900/0412.1961.2025.00091.

全文: PDF(3062 KB)  
摘要: 
目前异质金属4D打印仍处在概念设想阶段,对成形工艺选取、异质金属界面结合特性、热激励变形行为都缺乏探索。本工作开展了基于激光定向能量沉积技术的异质金属4D打印研究,考察了工艺参数和沉积方式对316L/Invar36合金界面平整性、界面成分过渡区以及构件热激励变形行为的影响。结果表明,当其它工艺参数一定时,在1000~1800 W的激光功率范围内,减小激光功率,可使316L与Invar36合金界面趋于平直,且成分过渡区宽度减小。在1000 W激光功率、15 mm/s扫描速率的条件下,当316L与Invar36合金按照上下排布方式进行沉积时,制备得到的板条状试样可在热激励下产生较大变形,且经历50 cyc热激励循环变形后形状仍可完全复原。当沉积方式为两种材料左右排布时,界面呈现锯齿状,且成分过渡区宽度增大,导致板条试样热激励变形显著降低。将两种材料以上下前后交替排布方式成形的板条试样,可在热激励下发生S状变形,将多个此种板条组装后,制备出一种能发生大幅变形的异质金属弹簧结构,其在270 ℃下可比25 ℃时伸长2.58倍。
关键词 4D打印异质双金属界面热激励变形    
Abstract

Heterogeneous metal 4D printing presents a promising technological route for fabricating structures with controllable thermally induced deformation. This approach addresses limitations inherent in shape memory alloy components, particularly their restricted number of stable deformation cycles, thereby offering broader application potential. Nonetheless, heterogeneous metal 4D printing remains at a conceptual stage, with limited research on process selection, interfacial bonding characteristics and thermally induced deformation behaviour. This study investigates the 4D printing of heterogeneous metals via laser solid forming of 316L/Invar36 alloys, focusing on the influence of process parameters and deposition configurations on interface flatness, compositional transition across the interface and thermally induced deformation. The results demonstrate that, with all other parameters held constant, decreasing the laser power within the 1000–1800 W range leads to a flatter interface and narrows the compositional transition zone between 316L and Invar36 alloys. At a laser power of 1000 W and scanning speed of 15 mm/s, strip-shaped specimens fabricated through vertical stacking of the two materials exhibit pronounced deformation under thermal actuation. In contrast, side-by-side deposition results in a jagged interface and a broader compositional transition zone, significantly diminishing the thermal actuation deformation of the resulting strip specimens. When 316L and Invar36 are alternately arranged in both vertical and horizontal orientations, the strips exhibit S-shaped deformation under thermal stimulation. Assembled from multiple such strips, a heterogeneous metal spring structure capable of substantial deformation is obtained, displaying a deformation magnitude 2.58 times greater at 270 °C than at 25 °C.


Key words4D printing    heterogeneous metals    interface    thermally induced deformation
收稿日期: 2025-04-02     
ZTFLH:  TG142  
基金资助:广东省重点领域研发计划项目
[1] 何家宝, 王亮, 张朝威, 邹明科, 孟杰, 王新广, 姜肃猛, 周亦胄, 孙晓峰. Al2O3 涂层对硅基陶瓷型芯与镍基单晶高温合金界面反应的影响[J]. 金属学报, 2025, 61(7): 1093-1108.
[2] 文恬恬, 岳继礼, 熊方宇, 袁媛, 黄光胜, 王敬丰, 潘复生. 可充电镁电池负极材料及界面化学的研究进展[J]. 金属学报, 2025, 61(3): 437-454.
[3] 贾春妮, 刘腾远, 郑成武, 王培, 李殿中. 中锰钢奥氏体中化学界面变形行为的晶体塑性研究[J]. 金属学报, 2025, 61(2): 349-360.
[4] 李振想, 王卫国, Rohrer Gregory S, 洪丽华, 陈松, 林燕, 周邦新. 室温和深冷轧制对纯Al再结晶{111}/{111}近奇异晶界的影响[J]. 金属学报, 2025, 61(11): 1673-1688.
[5] 王海丰, 蒲振新, 张建宝. 非平衡界面动力学理论[J]. 金属学报, 2025, 61(1): 29-42.
[6] 刘光辉, 王卫国, Rohrer Gregory S, 陈松, 林燕, 童芳, 冯小铮, 周邦新. 高温压缩变形Al-Zn-Mg-Cu合金动态再结晶后的{111}/{111}近奇异晶界[J]. 金属学报, 2024, 60(9): 1165-1178.
[7] 于云鹤, 谢勇, 陈鹏, 董浩凯, 侯纪新, 夏志新. 316L不锈钢表面激光熔化沉积CoCrNiCu中熵合金的界面相容性[J]. 金属学报, 2024, 60(9): 1213-1228.
[8] 王京京, 姚志浩, 张鹏, 赵杰, 张迈, 王蕾, 董建新, 陈迎. 镍基高温合金中S元素对基体与热障涂层界面稳定性的影响[J]. 金属学报, 2024, 60(9): 1250-1264.
[9] 张瑶, 齐敏, 孙佳, 吴婷, 马英杰, 王皞, 杨锐. 3D相场模拟研究Ti-6Al-4V合金片层组织形貌的影响因素[J]. 金属学报, 2024, 60(9): 1265-1278.
[10] 蒋招汉, 邱文婷, 龚深, 李周. 轻质高强高阻尼HfO2@CNT/聚合物/CuAlMn复合材料的制备及性能[J]. 金属学报, 2024, 60(3): 287-298.
[11] 董士虎, 张红伟, 吕文朋, 雷洪, 王强. 基于界面追踪-动网格技术模拟凝固收缩下Fe-C合金宏观偏析[J]. 金属学报, 2024, 60(3): 388-404.
[12] 冯小铮, 王卫国, Gregory S. Rohrer, 陈松, 洪丽华, 林燕, 王宗谱, 周邦新. 晶粒长大对高纯Al {111}/{111}近奇异晶界的影响[J]. 金属学报, 2024, 60(1): 80-94.
[13] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[14] 王宗谱, 王卫国, Rohrer Gregory S, 陈松, 洪丽华, 林燕, 冯小铮, 任帅, 周邦新. 不同温度轧制Al-Zn-Mg-Cu合金再结晶后的{111}/{111}近奇异晶界[J]. 金属学报, 2023, 59(7): 947-960.
[15] 王福容, 张永梅, 柏国宁, 郭庆伟, 赵宇宏. Al掺杂Mg/Mg2Sn合金界面的第一性原理计算[J]. 金属学报, 2023, 59(6): 812-820.