Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (2): 169-174    DOI:
Current Issue | Archive | Adv Search |
A MATHEMATICAL MODEL OF POST-COMBUSTION AT THE INITIAL STAGE IN TOP-BLOWN CONVERTER
LI Baowei; HE Youduo(Baotou institute of Iron and Steel;Baotou 014010);Y. SAHAI(The Ohio State University; USA)(Manuscript received 1995-05-30)
Cite this article: 

LI Baowei; HE Youduo(Baotou institute of Iron and Steel;Baotou 014010);Y. SAHAI(The Ohio State University; USA)(Manuscript received 1995-05-30). A MATHEMATICAL MODEL OF POST-COMBUSTION AT THE INITIAL STAGE IN TOP-BLOWN CONVERTER. Acta Metall Sin, 1996, 32(2): 169-174.

Download:  PDF(463KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the studies of the gas-flow, combustion and heat transfer in the top-blown converter, a general and coupling mathematical model has been proposed. The post-combustion ratio and heat-transfer efficiency in a 180t basic oxygen furnace (BOF) for the different design of oxygen lance were calculated by using this model. The obtained results are very important for understanding the post-combustion mechanism and improving the equipment of the post-combustion as well as raising the utilizing ratio of post-combustion heat. This model can be also extended to study the post-combustion at any time in the converter with a low foam slag layer.(Correspondent: LI Baowei, Department of Metallurgy, Baotou Institute of Iron and Steel, Baotou 014010)
Key words:  top-blown converter      post-combustion      heat transfer      mathematical model     
Received:  18 February 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I2/169

1HiraiM,TsujinoR,MukaiT,HaradaT,OmoriM,TransISIJ,1987;27B:8052GouH,IronsGA,LuWK.MetalTrans,1993;24:1793LiuyiZhang,OetersF,Steelresearch;l991;62(3):954李保卫,贺友多,SahaiY.包头钢铁学院学报,1994,13(4):305李保卫,贺友多,SahaiY.金属学报,1995;31:B145t
[1] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[2] TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan. Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control[J]. 金属学报, 2021, 57(10): 1229-1245.
[3] Shoumei XIONG, Jinglian DU, Zhipeng GUO, Manhong YANG, Mengwu WU, Cheng BI, Yongyou CAO. Characterization and Modeling Study on Interfacial Heat Transfer Behavior and Solidified Microstructure of Die Cast Magnesium Alloys[J]. 金属学报, 2018, 54(2): 174-192.
[4] Dunming LIAO, Liu CAO, Fei SUN, Tao CHEN. Research Status and Prospect on Numerical Simulation Technology of Casting Macroscopic Process[J]. 金属学报, 2018, 54(2): 161-173.
[5] Xiaoyu CHONG, Guangchi WANG, Jun DU, Yehua JIANG, Jing FENG. Numerical Simulation of Temperature Field and Thermal Stress in ZTAp/HCCI Composites DuringSolidification Process[J]. 金属学报, 2018, 54(2): 314-324.
[6] Chuansong WU, Hao SU, Lei SHI. Numerical Simulation of Heat Generation, Heat Transfer and Material Flow in Friction Stir Welding[J]. 金属学报, 2018, 54(2): 265-277.
[7] Heng SHAO,Yan LI,Hai NAN,Qingyan XU. RESEARCH ON THE INTERFACIAL HEAT TRANSFER COEFFECIENT BETWEEN CASTING AND CERAMIC SHELL IN INVESTMENT CASTING PROCESS OF Ti6Al4V ALLOY[J]. 金属学报, 2015, 51(8): 976-984.
[8] Yongyou CAO, Shoumei XIONG, Zhipeng GUO. DEVELOPMENT OF AN INVERSE HEAT TRANSFER MODEL BETWEEN MELT AND SHOT SLEEVE AND ITS APPLICATION IN HIGH PRESSURE DIE CASTING PROCESS[J]. 金属学报, 2015, 51(6): 745-752.
[9] WANG Xinxin, FAN Ding, HUANG Jiankang, HUANG Yong. NUMERICAL SIMULATION OF HEAT TRANSFER AND FLUID FLOW IN DOUBLE ELECTRODES TIG ARC-WELD POOL[J]. 金属学报, 2015, 51(2): 178-190.
[10] Xuewei YAN,Ning TANG,Xiaofu LIU,Guoyan SHUI,Qingyan XU,Baicheng LIU. MODELING AND SIMULATION OF DIRECTIONAL SOLIDIFICATION BY LMC PROCESS FOR NICKEL BASE SUPERALLOY CASTING[J]. 金属学报, 2015, 51(10): 1288-1296.
[11] LI Yan, FENG Yanhui, ZHANG Xinxin, WU Chuansong. A DYNAMIC HEAT SOURCE MODEL WITH RESPECT TO KEYHOLE EVOLUTION IN PLASMA ARC WELDING[J]. 金属学报, 2013, 49(7): 804-810.
[12] ZHANG Tao WU Chuansong CHEN Maoai. MODELLING FLUID FLOW AND HEAT TRANSFER PHENOMENA IN KEYHOLING STAGE OF PLASMA ARC WELDING[J]. 金属学报, 2012, 48(9): 1025-1032.
[13] CHENG Baisong, XIAO Namin, LI Dianzhong, LI Yiyi. SENSITIVITY ANALYSIS OF THE EFFECT OF INTERFACIAL HEAT TRANSFER COEFFICIENT ON DISTORTION SIMULATION DURING QUENCHING[J]. 金属学报, 2012, 48(6): 696-702.
[14] GAO Ao WANG Qiang LI Dejun JIN Baigang WANG Kai HE Jicheng. EFFICIENCY AND INFLUENCING FACTORS OF ELECTROMAGNETIC STEEL-TEEMING TECHNOLOGY[J]. 金属学报, 2010, 46(5): 634-640.
[15] YU Haiqi ZHU Miaoyong. NUMERICAL SIMULATION OF LIQUID STEEL SUPERHEAT REMOVAL IN SLAB CONTINUOUS CASTING MOLD[J]. 金属学报, 2009, 45(4): 476-484.
No Suggested Reading articles found!