FLOW STRESS OF BRASS AT HOT DEFORMATION
GUAN Kezhi; FAN Bailin; ZHOU Jihua(University of Science and Technology Beijing; Beijing 100083)(Manuscript received 1995-10-30; in revised form 1996-03-26)
Cite this article: 

GUAN Kezhi; FAN Bailin; ZHOU Jihua(University of Science and Technology Beijing; Beijing 100083)(Manuscript received 1995-10-30; in revised form 1996-03-26). FLOW STRESS OF BRASS AT HOT DEFORMATION. Acta Metall Sin, 1996, 32(7): 749-754.

Download:  PDF(401KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Flow stress curves of five types of brass were experimently studied with a cam plastometer at a constant deformed speed. The effects of the deformed temperature, determed rate and deformated degree to flow stress were analysed. At the same time, non-linear regressions to mathematical models with different structure were conducted. Through comparision and analysis, mathematical models with higher fitting accuracy were proposed.Correspondent: GUAN Kezhi, professor, Institute of Mechanical Engineering, University of Science and Technology Beijing, Beijing 100083
Key words:  brass      flow stress      mathematical model      cam plastometer     
Received:  18 July 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I7/749

1AM著,林治平译.金属与合金的塑性变形抗力手册.北京:机械工业出版社,1984:3322 管克智,周纪华,伦怡馨.钢铁,1989;24(9):273 刘志万.实验数据的统计分析和计算机处理.合肥:中国科学技术大学出版社,1989:1224 吴继庚.实用数值计算方法与程序.北京:冶金工业出版社,1991:129
[1] Xiangru GUO, Chaoyang SUN, Chunhui WANG, Lingyun QIAN, Fengxian LIU. Investigation of Strain Rate Effect by Three-Dimensional Discrete Dislocation Dynamics for fcc Single Crystal During Compression Process[J]. 金属学报, 2018, 54(9): 1322-1332.
[2] Dunming LIAO, Liu CAO, Fei SUN, Tao CHEN. Research Status and Prospect on Numerical Simulation Technology of Casting Macroscopic Process[J]. 金属学报, 2018, 54(2): 161-173.
[3] Tao WANG, Zhipeng WAN, Yu SUN, Zhao LI, Yong ZHANG, Lianxi HU. Dynamic Softening Behavior and Microstructure Evolution of Nickel Base Superalloy[J]. 金属学报, 2018, 54(1): 83-92.
[4] XUE Yingyu, TANG Jiancheng, ZHUO Haiou, YE Nan, WU Tong, ZHOU Xusheng. MICROSTRUCTURES AND PROPERTIES OF LEAD-FREE FREE-CUTTING GRAPHITE-BRASS PREPARED BY GRAPHITIZATION OF CEMENTITE[J]. 金属学报, 2015, 51(2): 223-229.
[5] Xuewei YAN,Ning TANG,Xiaofu LIU,Guoyan SHUI,Qingyan XU,Baicheng LIU. MODELING AND SIMULATION OF DIRECTIONAL SOLIDIFICATION BY LMC PROCESS FOR NICKEL BASE SUPERALLOY CASTING[J]. 金属学报, 2015, 51(10): 1288-1296.
[6] MO Yongda, JIANG Yanbin, LIU Xinhua, XIE Jianxin. MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF COLUMNAR-GRAINED HAl77-2 BRASS[J]. 金属学报, 2014, 50(11): 1367-1376.
[7] WEN Daosheng, ZONG Yingying, XU Wenchen, YANG Danmei, SHAN Debin. EFFECT OF 0.037%H ON HIGH TEMPERATURE DEFORMATION BEHAVIOR OF A CAST Ti-45Al-5Nb-0.8Mo-0.3Y ALLOY[J]. 金属学报, 2013, 49(11): 1428-1432.
[8] YU Hui KIM Youngmin YU Huashun YOU Bongsun MIN Guanghui. HOT DEFMATION BEHAVIOR AND HOT WORKABILITY OF Mg-Zn-Zr-Ce ALLOY[J]. 金属学报, 2012, 48(9): 1123-1131.
[9] SUN Chaoyang LUAN Jingdong LIU Geng LI Rui ZHANG Qingdong. PREDICTED CONSTITUTIVE MODELING OF HOT DEFORMATION FOR AZ31 MAGNESIUM ALLOY[J]. 金属学报, 2012, 48(7): 853-860.
[10] PAN Xiaolin WANG Bo SUN Wenru TU Ganfeng GUO Shouren HU Zhuangqi. EFFECT OF HOMOGENIZATION TREATMENT ON THE HOT DEFORMATION OF GH742 ALLOY[J]. 金属学报, 2012, 48(11): 1403-1408.
[11] SUN Chaoyang LIU Jinrong LI Rui ZHANG Qingdong. CONSTITUTIVE MODELING FOR ELEVATED TEMPERATURE FLOW BEHAVIOR OF INCOLOY 800H SUPERALLOY[J]. 金属学报, 2011, 47(2): 191-196.
[12] ZHANG Han BAI Bingzhe FANG Hongsheng. EFFECT OF PRESTRAIN ON THE SUPERPLASTIC DEFORMATION BEHAVIOR OF LOW-ALLOY HIGH-CARBON STEEL[J]. 金属学报, 2009, 45(9): 1106-1110.
[13] QIN YinJiang PAN Qinglin HE Yunbin LI Wenbin LIU Xiaoyan FAN Xi. HOT COMPRESSION BEHAVIOR AND FLOW STRESS PREDICTION OF ZK60 MAGNESIUM ALLOY[J]. 金属学报, 2009, 45(7): 887-891.
[14] KANG Mokuang ZHANG Mingxing LIU Feng ZHU Ming. OVERALL ACTIVATION ENERGY OF ISOTHERMAL TRANSFORMATION IN METAL ALLOY AND ITS MECHANISM II. Isothermal Transformation in β Brasses[J]. 金属学报, 2009, 45(1): 32-36.
[15] XiaoGuang Zhou. Modelling of Dynamic Recrystallization for Nb Bearing Steels on Flexible Thin Slab Rolling[J]. 金属学报, 2008, 44(10): 1188-1192 .
No Suggested Reading articles found!