| THE PRESENT CONDITION AND PROSPECTS ON METAL MATRIX COMPOSITES |
| WU Renjie (Shanghai Jiaotong University; Shanghai 200030) |
|
Cite this article:
WU Renjie (Shanghai Jiaotong University; Shanghai 200030). THE PRESENT CONDITION AND PROSPECTS ON METAL MATRIX COMPOSITES. Acta Metall Sin, 1997, 33(1): 78-84.
|
|
|
Abstract This article presents a review on the development condition of metal matrix composites (MMCs), includes its recent situations, varieties, production techniques, applications and existent problems. Some researching topics with great demand such as interface structure and behaviours, solidification, manufacturing science on some popular varieties of MMC and in situ technologies are also involved. On the base of these situations, a future development view is prospected.
|
|
Received: 18 January 1997
|
1吴人洁,复合材料学报,1987;41 2 Keily A Composites Sci Technol.1989;23:171 3 Lai S W,Chung D D L J Mater Sci 1994;29:3128 4 A J Cook Mater Sci Eng,1991;A144 5 Yue W,Lavernia E J JOM,1991;8:16 6Helmersson U, el al J Appl Phys,1987 62:481 7 Aronson R B.Machine Design,1985;8 68 8 Marsaden K JMetals 1985 6 59 9 Allison J E,Cole G S.JOM,1993;45:19 10吴人洁,李鹏兴 见:李恒德,肖纪美主编,材料的表面与界面,北京;清华大学出版社,1990 11储双杰,吴人活电子显微学报,1996,待发表 12王浩伟,储双杰,张国定,吴人洁 机械工程学报,1996;31(1):97 13 Wu R J Proceedings of ICCM 6 &ECCM-2 1987;2:128 14 Fulcunaga H,Komatsu S,Kanoh Y Bull Jpn Soc Mech Eng,1983;26;1814 15 Stefanesu D M,Dhindars B K,et al.Metall Trans 1988;19A:2847 16储双杰,金瑞,王浩伟,吴人洁,赵昌正.有色金属,1996 待发表 17储双杰,吴人洁.金属学报,待发表 18Stefanescu D M.Key Eng Mater,1993;79-80:74 19谢国宏.材料工程,1994(12):5 20Clyne T W,Bader M G.Proc of International Conference on Composite Materials TMS-ALME,1985:755 21Doncel G G,Karmarker S D,Divecha A P,Sherby O D Composile Sci Tech 1989; 35:105 22 Schuster D JOM,1993;45:26 23 Newkirk M S Ukgnhart A W.J Mater Res,1986;1:8 24 Denillmnscat T,Robin A L.Metall Trans ,1994 25A:2357 25 Clear T D,Johnson W B. Ceram Eng Sci Proc,1989;10:7 26 崔容翔,吴人洁 金属学报,1996;32 101p |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|