PHYSICAL-CHEMISTRY EFFECT OF RARE EARTH ELEMENTS ON METALLIC MATERIALS
DU Ting (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081)
Cite this article: 

DU Ting (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081). PHYSICAL-CHEMISTRY EFFECT OF RARE EARTH ELEMENTS ON METALLIC MATERIALS. Acta Metall Sin, 1997, 33(1): 69-77.

Download:  PDF(851KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The phase equilibria and thermodynamic parameters, as a function of temperature, of twenty nine ternary and quaternary Fe-base metallic systems containing one of representative elements (Ce, Y, La, Nd, Sm) and S, O, S+O, C, N, Sb, Sn, Pb, P, Cu, Ti, Nb,V respectively, of seven Ni-base metallic systems containg one of the Ce, Y, La elements and S, O, S+O solute element, of twenty Cu-base metallic systems containing Ce or Y and S, O,S+O, Al, Si, Pb, Sn, Zn, Ti, Fe solute element respectively, of ten Al-base metallic systems containing Ce and Mg, Ti, Mn, Zn, Fe, Sn, Pb, Ni, Cu, Si, S solute element respectively were determined by different experimental meth0ds according to the cheracter of systems. The dynamic parameters between rara earth addition agents and S, O, N, H in iron-steel liquid solutions and the data for the effect and application of rare earths in more twenty alloys were obtained. These results of author's group provide a basis for explaining summarily some physic-chemistry effect of rare earth elements on metals and alloys.
Key words:  rare earth elements      metallic materials      physic-chemistry effect     
Received:  18 January 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I1/69

1杜挺.科学通报,1963:13
2杜挺.中国金属学会炼钢委员会1980年年会炼钢论文集.武汉钢铁公司,1982
3杜挺,韩其勇,王常珍稀土碱土等元素的物理化学及在材料中的应用北京:科学出版社,1995
4杜挺中国稀土学会第H届学术年会论文集第3分册,1990:24
5社挺,李国栋金属学报,1993;29:B316
6Du Ting, Wang Longmei, Wu Yieming Inorganica Chimica Acta 1987 140: 187
7吴夜明,杜挺钢铁研究总院学报,1985 5:137
8 Du Ting,Wang Longmei,Wu Yieming etc J Mater Sci Technol,1993;9:68
9王龙妹,杜挺金属学报,1984 20: A286 1985;21:A289 1987 23:B283
10李国栋,杜挺金属学报,1991;27: B286 Acta Metall Sin,1992;5B:68
11 Du Ting,Wang Longmei J Less-Common Met ,1985;110:179
12王龙妹,杜挺钢铁,1985;20(8):9
13王龙妹,杜挺,吴夜明。稀土, 1987;(6):11
14杜挺,乐可襄金属学报,1991;23:B213
15唱鹤鸣,杜挺,余景牛金属学报,1989;25:B140,Acta Metall Sin 1989;2B:364
16周谦利,杜挺金属学报,1989;25 Bll,Acta Melall Sin、1989;2B:235
17 Du Ting etc J Alloy COmpounds,1993;193:38
18杜挺物理1990;(1);27
19乐可襄,社挺,李继宗,沈汝美金属学报,1987;23:A99
20杜挺钢铁研究学报, 1994 6(3): 6
21周谦利,杜挺中国稀土学报, 1990; 8(2):114
22王正跃,王龙妹,杜挺.金属学报,1988;24:B170,Acta Metall Sin,1988;1B:199
23 社 挺,余宗森等钒钛锡等微合金元素在低合金钢中应用基础的研究北京:科学技术出版社,1992:216
24王跃奎,杜挺金属学报,1990;25:B222
25杜挺,孙运涌,吴夜明中国稀土学会第三届学术年会论文集第3分册,1994:101,化工冶金,1995;16(3):189
26杜挺,李国栋化工冶金,1994;15(3);214
27杜挺,李国栋中国有色金属学报,1994 4(3):25,1994 2(4):45
28杜挺,李国栋金属学报,1993;29:B316
29 Du Ting,Li Guodong.Tr ans Nonferrous Met Society of China,1994;4(3):17
30 Du Thg,Li Guokong Trans Nonferrous Met Society of China,1995;5(3):16D
[1] XU Songbo;CHEN Junming (Shanghai Institute of Metallurgy; Chinese Academy of Sciences)(Manuscript received 5 July; 1993; in revised form 6 September 1993). AN IMPROVEMENT OF ROOM TEMPERATURE DUCTILITY OF Ni_3Al(B)-Cr BASE ALLOYS BY MULTI-ALLOYING OF Mg AND RE[J]. 金属学报, 1994, 30(5): 221-224.
No Suggested Reading articles found!