| SPECIFIC HEAT AND KAUZMANN TEMPERATURE OF PtNiP ALLOY |
| JIANG Qing;XU Xiaoya; Li Jianchen (Jilin University of Technology; Changchun130025) |
|
Cite this article:
JIANG Qing;XU Xiaoya; Li Jianchen (Jilin University of Technology; Changchun130025). SPECIFIC HEAT AND KAUZMANN TEMPERATURE OF PtNiP ALLOY. Acta Metall Sin, 1997, 33(6): 660-666.
|
|
|
Abstract The Kauzmann temperature and the reverse Kauzmann temperature of thePt69.0Ni9.6P21.4 alloy are determined by use of the measured specific heat functions and thecorresponding entropy functions of the alloy. The obtained Kauzmann temperature is consistent to that calculated by Vogel-Fulcher law and by the melting points of the components ofthe alloy. During the measurements of the specific heat of the undercooled liquid, differentheating rates are utilized to enlarge the measuring temperature range nearby the glass transition temperature. Thus the reliability of the thermodynamic function of the undercooled liquid is increased. The possibility for the overheating of the crystal is studied by producing oxide films on the surface of the crystalline specimen.
|
|
Received: 18 June 1997
|
1Johnson W L.Prog Mater Sci,1986;30:81 2Fecht H J.Johnson W L. Nalure, 1988; 334: 50 3Cahn W. Nature, 1986: 323: 668 4 Kauzmann W. Chem Rev, 1948; 43: 219 5 Wolf D,Okamoto P R,Yip S,Lutsko J F,Kluge M.J Mater Res.1990;5:286 6 fecht H J. Nature, 1992; 356: 133 7 Chen H S.J Non-Cryst Solids,1973:12:333 8Inoue A,Zhang T,Masumoto T.JNon-Cryst Solids,1993-156-158:473 9 Chen H S.Acta Metall.1974;22:1505 10 Jiang Q,Li J C,Tong J.Mater Sci Eng,1995;A196,165 11卢柯.金属学报,1992;28:B17 12Bergman C, Komarek K L. Calphad, 1985; 9(1): 1 13 Agren J,Cheynet B.Clavaguera-Mora M T,Hack K,Hertz J,Sommer F,Kattner U.Calphad,1995:19:449 14蒋青,徐晓亚,赵明.金属学报,1997;33待发表 15 Saslow W S Phys Rev B, 1988; 37: 676 16 Bruning R,Samwer K.Phys Rev B,1992;46:11318 17 Klose G、Fecht J H.Mater Sci Eng,1994;A179/180:77) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|