SPECIFIC HEAT AND KAUZMANN TEMPERATURE OF PtNiP ALLOY
JIANG Qing;XU Xiaoya; Li Jianchen (Jilin University of Technology; Changchun130025)
Cite this article: 

JIANG Qing;XU Xiaoya; Li Jianchen (Jilin University of Technology; Changchun130025). SPECIFIC HEAT AND KAUZMANN TEMPERATURE OF PtNiP ALLOY. Acta Metall Sin, 1997, 33(6): 660-666.

Download:  PDF(1483KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The Kauzmann temperature and the reverse Kauzmann temperature of thePt69.0Ni9.6P21.4 alloy are determined by use of the measured specific heat functions and thecorresponding entropy functions of the alloy. The obtained Kauzmann temperature is consistent to that calculated by Vogel-Fulcher law and by the melting points of the components ofthe alloy. During the measurements of the specific heat of the undercooled liquid, differentheating rates are utilized to enlarge the measuring temperature range nearby the glass transition temperature. Thus the reliability of the thermodynamic function of the undercooled liquid is increased. The possibility for the overheating of the crystal is studied by producing oxide films on the surface of the crystalline specimen.
Key words:  Pt_(69.0)Ni_(9.6)P_(21.4) alloy      specific heat      Kauzmann temperature     
Received:  18 June 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I6/660

1Johnson W L.Prog Mater Sci,1986;30:81
2Fecht H J.Johnson W L. Nalure, 1988; 334: 50
3Cahn W. Nature, 1986: 323: 668
4 Kauzmann W. Chem Rev, 1948; 43: 219
5 Wolf D,Okamoto P R,Yip S,Lutsko J F,Kluge M.J Mater Res.1990;5:286
6 fecht H J. Nature, 1992; 356: 133
7 Chen H S.J Non-Cryst Solids,1973:12:333
8Inoue A,Zhang T,Masumoto T.JNon-Cryst Solids,1993-156-158:473
9 Chen H S.Acta Metall.1974;22:1505
10 Jiang Q,Li J C,Tong J.Mater Sci Eng,1995;A196,165
11卢柯.金属学报,1992;28:B17
12Bergman C, Komarek K L. Calphad, 1985; 9(1): 1
13 Agren J,Cheynet B.Clavaguera-Mora M T,Hack K,Hertz J,Sommer F,Kattner U.Calphad,1995:19:449
14蒋青,徐晓亚,赵明.金属学报,1997;33待发表
15 Saslow W S Phys Rev B, 1988; 37: 676
16 Bruning R,Samwer K.Phys Rev B,1992;46:11318
17 Klose G、Fecht J H.Mater Sci Eng,1994;A179/180:77)
[1] Tingting JIA,Zengyun JIAN,Junfeng XU,Man ZHU,Fang'e CHANG. CHARACTERISTIC TEMPERATURE AND PERFOR-MANCE OF THE Ge30Se70 CHALCOGENIDE GLASS[J]. 金属学报, 2016, 52(6): 755-760.
[2] Jiaojiao LI,Zengyun JIAN,Man ZHU,Junfeng XU,Fang'e CHANG,Min XIANG. STUDY ON THERMODYNAMIC PROPERTIES AND KINETICS FRAGILITY OF GexSe90-xSb10 CHALCOGENIDE GLASSES[J]. 金属学报, 2015, 51(11): 1384-1390.
[3] WEI Bingbo; WANG Bin(Northwestern Polytechnical University; Hi'an)BARTH M;HERLA CH D M(Institut for Raumsimulation; DLR; Germany). THERMODYNAMIC DRIVING FORCE FOR RAPID CRYSTALLIZATION OF LIQUID METALS[J]. 金属学报, 1994, 30(19): 289-293.
[4] TONG Huayu;DING Bingzhe;JIANG Honggang;LI Shuling;LI Gusong;WANG Jingtang State Key Laboratory of RSA; Institute of Metal Research; Academia Sinica; Shenyang Correspondent Research assistant; Institute of Metal Research; Academia Sinica; Shenyang 110015. THERMAL PROPERTIES OF NANOCRYSTALLINE Fe_(78)B_(13)Si_9 ALLOY[J]. 金属学报, 1992, 28(6): 71-75.
[5] WEI Bingbo;YANG Gencong;ZHOU Yaohe Northwestern Polytechnical University; Xi'an. DENUCLEATION AND HIGH UNDERCOOLING OF Ni-32.5%Sn EUTECTIC ALLOY[J]. 金属学报, 1990, 26(5): 119-124.
[6] SHEN Tao; WANG Jingtang Institute of Metal Research Academia Sinica; Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Shenyang professor. VARIATIONAL CALCULATION OF THERMODYNAMIC PROPERTIES OF SUPERCOOLED LIQUID METALS[J]. 金属学报, 1990, 26(3): 119-125.
No Suggested Reading articles found!