| MECHANISM FOR THE OCCURRENCE OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS |
| TIAN Boohui(Beliing Institute of Aeronautical Materials; Beijing 100095)LI Huanxi; ZHANG Youggang; CHEN Changqi(Beijing University of Aeronautics and Astronautics; Beijing 100083)Corresponent: TIAN Baohui; Tel: (010)62456622-5021 Fax:(010)62456925 |
|
Cite this article:
TIAN Boohui(Beliing Institute of Aeronautical Materials; Beijing 100095)LI Huanxi; ZHANG Youggang; CHEN Changqi(Beijing University of Aeronautics and Astronautics; Beijing 100083)Corresponent: TIAN Baohui; Tel: (010)62456622-5021 Fax:(010)62456925. MECHANISM FOR THE OCCURRENCE OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS. Acta Metall Sin, 1998, 34(6): 603-608.
|
|
|
Abstract Strain rate sensitivity varies in a different mariner in Al-Li single crystalsunder different ageing conditions. Stress drops change irregularly with increasing strain andbear no relation to elapsed time for individual serrations. Stress drops and elapsed time duringserrated flow Primarily distribute within their low values under peak aged condition, comparedwith underaged and overaged states. These behaviors may be explained by sheared σ' particlesinducling serrated flow.
|
|
Received: 18 June 1998
|
1 Behnood N, Evans J T. Acta Metall 1989; 37: 687 2 Kumars,Krol J,Pink E.Scr Mater 1996;35:775 3 Ilic N, Drobnjak Dj, Radmilovic V, Jovanovic M T, Markovic D. Ser Mater 1996; 34: 1123 4 田宝辉,李焕喜,张永刚,陈昌麒.金属学报,1997;33:577 (Tian B H, Li H X, Zhang Y G, Chen C Q. Acta Metall Sin, 1997; 33: 577) 5 Kocks U F ,Cook R E,Mulford R A.Acta Metall 1985;33:623 6 McCormick P G. Acto Metall 1972; 20: 351 7 Hong K T, Nam S W. Acta Metal 1989; 37: 31 8 Diego N,Rio J del ,Segers D,Dorkens-Vapraet L,Dorikens M.Phy Rev 19930;B48:6781 9 Harun H J ,McCormick P G ,Acta Metall ,1979;27:155 10 McCormick P G. Acta Metall, 1971; 19: 463 11 Pink E, Grinberg A. Acta Metal 1982; 30: 2153 12 Fujita H, Tanata T. Acta Metall, 1977; 25: 793 13 Kumar S and Pink E.Acta Mater 1997;45:5205 14 Brechet Y ,Estrin Y.Scr Metall Mater 1994;31:185 |