MOLECULAR DYNAMICS SIMULATION ON MARTENSITIC NUCLEATION AND GROWTH AT AN EDGE DISLOCATION DIPOLE
LI Bin; ZHANG Xiumu; LI Rong; LI Yiyi(Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: ZHANG Xiumu; professor Tel: (024)22843531-55362; Fax: (024)23891320;E-mail: xmzhang imr. ac. cn
Cite this article: 

LI Bin; ZHANG Xiumu; LI Rong; LI Yiyi(Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: ZHANG Xiumu; professor Tel: (024)22843531-55362; Fax: (024)23891320;E-mail: xmzhang imr. ac. cn. MOLECULAR DYNAMICS SIMULATION ON MARTENSITIC NUCLEATION AND GROWTH AT AN EDGE DISLOCATION DIPOLE. Acta Metall Sin, 1998, 34(8): 813-818.

Download:  PDF(545KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Molecular dynamics simulation has been performed to investigate martensite nucleation and growth at an edge dislocation dipole employing embedded atom method (EAM) type interatomic potential. The results indicate that the stress field of the dislocation dipole has important effect on the martensite nucleation and growth. The calculation of the stress distribution of the dislocation dipole shows that martensitic nucleation was preferentially initiated at the sites in the stress field where the stress state assists the lattice deformation of martensitic transformation. The two dislocations moved apart gradually, driven by transformation strain during the growing process of the martensite. The slip of the dislocation plays a role of plastic accommodation.
Key words:  molecular dynamics simulation      edge dislocation dipole      EAM potential      martensitic nucleation and growth      stress field     
Received:  18 August 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I8/813

1 Magee C L. Metall Trans, 1971; 2: 2419
2 Clapp P C. Phys Status Solid. 1973; 57(B): 561
3 Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897, 1905, 1915
4 Kajiwara S. Metall Trans, 1986; 17A: 1701
5 Easterlillg K E, Tholen A R. Acta Metall, 1976; 24: 333
6 Daw M S, Baskes M I. Phys Rev Lett, 1983; 50: 1285
7 Daw M S, Baskes M I. Phys Rev, 1984; 29B: 6443
8 Chen S P, Scrolovitz D J, Voter A F. J Mater Res, 1989; 4: 62
9 Clapp P C, Rifkin J. Mat Res Soc Proc, 1984; 21: 643
10 Yu Z Z, Clapp P C. Metall Trans, 1989; 28: 685
11 Rifkin J, Clapp P C. i Phys Colloq, 1982; C4: 157
12沙宪伟,张修睦,陈魁英,李依依金属学报,1996;32:685(Sha X W, Zhang X M, Chen K Y, Li Y Y. Acta Metall Sin, 1996 32: 685)
13沙宪伟,张修睦,李依依材料研究学报,1997;11:280(Sha X W, Zhang X M, Li Y Y. Chin J Moter Res, 1997; 11: 280)
14沙宪伟,张修睦,李斌,李依依金属学报1997; 33:1(Sha X W, Zhang X M, Li B, Li Y Y Acta Metall Sin, 1997; 33: 1)
[1] LIANG Jinjie, GAO Ning, LI Yuhong. Interaction Between Interstitial Dislocation Loop and Micro-Crack in bcc Iron Investigated by Molecular Dynamics Method[J]. 金属学报, 2020, 56(9): 1286-1294.
[2] ZHOU Xia,LIU Xiaoxia. Mechanical Properties and Strengthening Mechanism of Graphene Nanoplatelets Reinforced Magnesium Matrix Composites[J]. 金属学报, 2020, 56(2): 240-248.
[3] DUAN Lingjie,LIU Yongchang. Relationships Between Elastic Constants and EAM/FS Potential Functions for Cubic Crystals[J]. 金属学报, 2020, 56(1): 112-118.
[4] Haifeng ZHANG, Haile YAN, Nan JIA, Jianfeng JIN, Xiang ZHAO. Exploring Plastic Deformation Mechanism of MultilayeredCu/Ti Composites by Using Molecular Dynamics Modeling[J]. 金属学报, 2018, 54(9): 1333-1342.
[5] LIANG Li, MA Mingwang, TAN Xiaohua, XIANG Wei, WANG Yuan, CHENG Yanlin. A SIMULATION STUDY OF MECHANICAL PROPER-TIES OF METAL Ti SAMPLE WITH DEFECTS[J]. 金属学报, 2015, 51(1): 107-113.
[6] KE Changbo, CAO Shanshan, MA Xiao, HUANG Ping, ZHANG Xinping. PHASE FIELD SIMULATION OF AUTO-CATALYTIC GROWTH EFFECT OF COHERENT Ni4Ti3 PRECIPITATE IN NiTi SHAPE MEMORY ALLOY[J]. 金属学报, 2013, 49(1): 115-122.
[7] MO Yunfei, LIU Rangsu, LIANG Yongchao, ZHENG Naichao, ZHOU Lili,TIAN Zean, PENG Ping. MOLECULAR DYNAMICS SIMULATION ON THE EVOLUTION OF MICROSTRUCTURES OF LIQUID ZnxAl100−x ALLOYS DURING RAPID SOLIDIFICATION[J]. 金属学报, 2012, 48(8): 907-914.
[8] GAO Yufei MENG Qingyuan. MOLECULAR DYNAMICS SIMULATION ON THERMAL CONDUCTIVITY OF ONE DIMENISON NANOMATERIALS[J]. 金属学报, 2010, 46(10): 1244-1249.
[9] LIU Xiaoming YOU Xiaochuan LIU Zhanli NIE Junfeng ZHUANG Zhuo. MOLECULAR DYNAMICS SIMULATION OF PLASTIC BEHAVIOR OF THE Ni NANOFILM DURING SCRATCH PROCESS[J]. 金属学报, 2009, 45(2): 137-142.
[10] ZHANG Tao; ZHANG Xiaoru; GUAN Li; QI Yuanhua; XU Changye. The Simulation of Metal Cu In The Melting and Solidification Process[J]. 金属学报, 2004, 40(3): 251-256 .
[11] LI Qikai; ZHANG Yue; CHU Wuyang. MOLECULAR DYNAMICS SIMULATION OF PLASTIC DEFORMATION DURING NANOINDENTATION[J]. 金属学报, 2004, 40(12): 1238-1242 .
[12] WANG Luhong; LIU Haozhe; HU Zhuangqi (State Key Lab of BSA; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: WANG Luhong; Tel. (024)23843531-55405(O); (024)25842383(H). SIMULATION OF LIQUID STATE STRUCTURES AND RAPID SOLIDIFICATION OF METALS[J]. 金属学报, 1998, 34(9): 933-938.
[13] LI Bin;ZHANG Xiumu; SHA Xianwei; LI Yiyi (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: LI Bin; Tel: (024)23843531-55362; Fax: (024)23891320. MOLECULAR DYNAMICS SIMULATION ON TRANSFORMATION PSEUDOELASTICITY IN NiAI ALLOY[J]. 金属学报, 1998, 34(9): 923-927.
[14] HU Wangyu; GUAN Hengrong; SUN Xiaofeng; LI Shizhuo; FUKUMOTO Masahiro;OKANE Isao(Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Department of Applied Physics; Hunan University; Changsha 410082)(Toyobashi University of Technology Toyobashi; Japan)Correspondent: SUN Xiaofeng; associate profssor Tel: (024)23843531-55608; Fax: (024)23891320. THERMAL SHOCK BEHAVIOR OF ZrO_2/Ni GRADED THERMAL BARRIER COATINGS[J]. 金属学报, 1998, 34(10): 1104-1114.
[15] SHA Xianwei;ZHANG Xiumu;LI Bin;LI Yiyi(Institute of Metal Research;The Chinese Academy of Sciences;Shenyang 110015). MOLECULAR DYNAMICS STUDY ON THE INFLUENCE OF SINGLE EDGE DISLOCATION ON MARTENSITIC TRANSFORMATIONS IN NiAl[J]. 金属学报, 1997, 33(11): 1121-1129.
No Suggested Reading articles found!