Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (10): 1247-1252     DOI:
Research Articles Current Issue | Archive | Adv Search |
Effect of La on the corrosion morphology of AZ91
Wu Guohua
上海交通大学;材料学院
Cite this article: 

Wu Guohua. Effect of La on the corrosion morphology of AZ91. Acta Metall Sin, 2008, 44(10): 1247-1252 .

Download:  PDF(2520KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure, corrosion morphology and corrosion product of AZ91D and AZ91D-1.0La alloy were investigated. With the addition of 1% La in AZ91D, not only rod-like Al11La3 and blocky Al8LaMn4 phase, but also more fine laminar β phase-Mg17Al12 around large β phase particles formed. The fine laminar β phase obviously restrained the further development of corrosion, which greatly improved the corrosion resistance of AZ91D. Al11La3 phase was cathodic phase, but this phase did not accelerate corrosion of α matrix because Al11La3 was rod-like phases, which only offered a small cathodic area. However, blocky Al10Ce2Mn7 phase obviously accelerated corrosion of α matrix because of its large cathadic area. Al11La3 and Al8LaMn4 are corrosion resistant phases, but they could not restrain the development of corrosion because their distribution was not continuous.
Key words:       
Received:  22 October 2007     
ZTFLH:  TG146.2  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I10/1247

[1]Andreatta F,Apachitei I,Kodentsov A A,Dzwonczyk J, Duszczyk J.Electrochim Acta,2006;51:3551
[2]Lafront A M,Zhang W,Jin S,Tremblay R,Dube D,Ghali E.Electrochim Acta,2005;51:489
[3]Mathieu S,Rapin C,Hazan J,Steinmetz P.Corros Sci, 2002;44:2737
[4]Song G,Atrens A,St John D,Wu X,Nairn J.Corros Sci, 1997;39:1981
[5]Ambat R,Aung N N,Zhou W.Corros Sci,2000;42:1433
[6]Song G,Atrens A,Dargush M.Corros Sci,1999;41:249
[7]Song G,Bowles A L,Stjohn D H.Mater Sci Eng,2004; A366:74
[8]Song G.Atrens A.Adv Eng Mater,1999;1:11
[9]Fan Y,Wu G,Gao H,Zhai C.J Electrochem Soc,2006; 153:B283
[10]Fan Y,Wu G,Gao H,Zhai C.Mater Sci Forum,2005; 488:869
[11]Wu G,Fan Y,Gao H,Zhai C,Zhu Y.Mater Sci Eng, 2005;A408:255
[12]Aung N N,Zhou W J.Appl Electrochem,2002;32:1397
[13]Jinko Y,Yim C D,Lim J D.Mater Sci Forum,2003;419- 422:851
[14]Morales E D,Ghali E,Hort N,Dietzel W,Kainer K U. Mater Sci Forum,2003;419:867
[15]Song G,St John D.J Light Metals,2002;2:1
[16]Huang Z H,Guo X F,Zhang Z M,Xu C J.Acta Metall Sin(Engl Lett),2005;18:129
[17]Fan Y,Wu G,Zhai C.Mater Sci Eng,2006;A433:208
[18]Fan Y,Wu G H,Gao H T,Li G Q,Zhai C Q.Acta Metall Sin,2006;42:35 (樊昱.吴国华,高洪涛,李冠群.翟春泉.金属学报,2006;42:351
[19]Lunder O,Lein J E,Aune T,Nisancioglu K.Corrosion, 1989;45:741
[20]Song G,Atrens A,Wu X,Zhang B.Corros Sci,1998;40: 1769
[21]Lunder O,Nisancioglu K,Hansen R S.SAE Technical Paper Series No.930755,Soc.Automotive Eng.,Detroit, 1993:867
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!