| Effect of La on the corrosion morphology of AZ91 |
| Wu Guohua |
| 上海交通大学;材料学院 |
|
Cite this article:
Wu Guohua. Effect of La on the corrosion morphology of AZ91. Acta Metall Sin, 2008, 44(10): 1247-1252 .
|
|
|
Abstract The microstructure, corrosion morphology and corrosion product of AZ91D and AZ91D-1.0La alloy were investigated. With the addition of 1% La in AZ91D, not only rod-like Al11La3 and blocky Al8LaMn4 phase, but also more fine laminar β phase-Mg17Al12 around large β phase particles formed. The fine laminar β phase obviously restrained the further development of corrosion, which greatly improved the corrosion resistance of AZ91D. Al11La3 phase was cathodic phase, but this phase did not accelerate corrosion of α matrix because Al11La3 was rod-like phases, which only offered a small cathodic area. However, blocky Al10Ce2Mn7 phase obviously accelerated corrosion of α matrix because of its large cathadic area. Al11La3 and Al8LaMn4 are corrosion resistant phases, but they could not restrain the development of corrosion because their distribution was not continuous.
|
|
Received: 22 October 2007
|
|
|
[1]Andreatta F,Apachitei I,Kodentsov A A,Dzwonczyk J, Duszczyk J.Electrochim Acta,2006;51:3551 [2]Lafront A M,Zhang W,Jin S,Tremblay R,Dube D,Ghali E.Electrochim Acta,2005;51:489 [3]Mathieu S,Rapin C,Hazan J,Steinmetz P.Corros Sci, 2002;44:2737 [4]Song G,Atrens A,St John D,Wu X,Nairn J.Corros Sci, 1997;39:1981 [5]Ambat R,Aung N N,Zhou W.Corros Sci,2000;42:1433 [6]Song G,Atrens A,Dargush M.Corros Sci,1999;41:249 [7]Song G,Bowles A L,Stjohn D H.Mater Sci Eng,2004; A366:74 [8]Song G.Atrens A.Adv Eng Mater,1999;1:11 [9]Fan Y,Wu G,Gao H,Zhai C.J Electrochem Soc,2006; 153:B283 [10]Fan Y,Wu G,Gao H,Zhai C.Mater Sci Forum,2005; 488:869 [11]Wu G,Fan Y,Gao H,Zhai C,Zhu Y.Mater Sci Eng, 2005;A408:255 [12]Aung N N,Zhou W J.Appl Electrochem,2002;32:1397 [13]Jinko Y,Yim C D,Lim J D.Mater Sci Forum,2003;419- 422:851 [14]Morales E D,Ghali E,Hort N,Dietzel W,Kainer K U. Mater Sci Forum,2003;419:867 [15]Song G,St John D.J Light Metals,2002;2:1 [16]Huang Z H,Guo X F,Zhang Z M,Xu C J.Acta Metall Sin(Engl Lett),2005;18:129 [17]Fan Y,Wu G,Zhai C.Mater Sci Eng,2006;A433:208 [18]Fan Y,Wu G H,Gao H T,Li G Q,Zhai C Q.Acta Metall Sin,2006;42:35 (樊昱.吴国华,高洪涛,李冠群.翟春泉.金属学报,2006;42:351 [19]Lunder O,Lein J E,Aune T,Nisancioglu K.Corrosion, 1989;45:741 [20]Song G,Atrens A,Wu X,Zhang B.Corros Sci,1998;40: 1769 [21]Lunder O,Nisancioglu K,Hansen R S.SAE Technical Paper Series No.930755,Soc.Automotive Eng.,Detroit, 1993:867 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|