Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (7): 843-847     DOI:
Research Articles Current Issue | Archive | Adv Search |
Microstructure transition from primary ε phase to peritectic η phase in Cu-75%Sn peritectic alloy under laser rapid solidification
西北工业大学大学凝固技术国家重点实验室
Cite this article: 

. Microstructure transition from primary ε phase to peritectic η phase in Cu-75%Sn peritectic alloy under laser rapid solidification. Acta Metall Sin, 2008, 44(7): 843-847 .

Download:  PDF(2108KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  06 December 2007     
ZTFLH:  TG132.32  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I7/843

[1]Umeda T,Okane T,Kurz W.Acts Mater,1996;44:4209
[2]Vandyoussefi M,Kerr H W,Kurz W.Acts Mater,2000; 48:2297
[3]Ma D,Li Y,Ng S C,Jones H.Acts Mater,2000;48:1741
[4]Su Y Q,Liu C,Li X Z,Guo J J,Li B S,Jia J,Fu H Z. Intermetallics,2005;13:267
[5]Shibata H,Arai Y,Suzuki M,Emi T.Metall Mater Trans, 2000;31B:981
[6]Li S M,Ma B L,LüH Y,Liu L,Fu H Z.Acts Metall Sin, 2005;41:411 (李双明,马伯乐,吕海燕,刘林,傅恒志.金属学报,2005;41:411)
[7]LüH Y,Li S M,Liu L,Fu H Z.Spec Cast Nonferrous Alloys,2006;26:753 (吕海燕,李双明,刘林,傅恒志.特种铸造及有色合金,2006;26:753)
[8]LüH Y,Li S M,Liu L,Fu H Z.Sci China,2007;50G:451
[9]Su Y P,Wang M,Lin X,Li H L,Huang W D.Acts Metall Sin,2005;41:67 (苏云鹏,王猛,林鑫,李华琳,黄卫东.金属学报,2005;41:67)
[10]Xu W,Feng Y P,Li Y,Zhang G D,Li Z Y.Acts Mater, 2002;50:183
[11]Duan G H,Liu Y C,Yang G C,Zhou Y H.Mater Left, 2003;57:1091
[12]Kerr H W,Kurz W.Int Mater Rev,1996;41:129
[13]Kubin L P,Estrin Y.Acts Metall,1985;33:397
[14]Kurz W,Fisher D J.Fundamentals of Solidification.4th Ed.,Switzerland:Trans Tech Publications Ltd,1998:201
[15]Trivedi R,Kurz W.Metall Trans,1990;21A:1311
[16]Fredriksson H,Nylen T.Met Sci,1982;16:283
[17]Saunders N,Miodownik A P.Phase Diagrams of Binary Copper Alloys.Materials Park,OH:ASM International, 1994:412
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!