“SEAWEED”MORPHOLOGY IN Fe--Sn--Si TERNARY MONOTECTIC ALLOY
REN Lina; CAI E; FENG Sheng
Northwest Institute for Non--Ferrous Metal Research
Cite this article: 

REN Lina; CAI E; FENG Sheng. “SEAWEED”MORPHOLOGY IN Fe--Sn--Si TERNARY MONOTECTIC ALLOY. Acta Metall Sin, 2008, 44(3): 307-313 .

Download:  PDF(1270KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  03 July 2007     
ZTFLH:  TG132  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I3/307

[1]Creuze J,Bertheer F,Tetor R,Legrand B.Phys Rev Lett, 2001;86:5735
[2]Wang N,Wei B.Mater Sci Eng,2003;A345:145
[3]Blum B,Hammer L,Schmidt Ch,Schmidt C,Meier W, Wieckhorst O,Muller S,Heinz K.Phys Rev Lett,2002; 89:266102
[4]Creuze J,Berthier F,Tetot R Legrand B.Phys Rev Lett, 2001;86:5735
[5]Akamatsu S,Faivre G,Ihle T.Phys Rev,1995;5E:4751
[6]Utter B,Ragnarsson R,Bodenschatz E.Phys Rev Lett, 2001;86:4604
[7]Ihle T,Muller-Krumbhaar H.Phys Rev Lett,1993;70: 3083
[8]McCloud K,Maher J.Phys Rep,1995;260:139
[9]Matsuyama T,Matsushita M.Crit Rev Microbiol,1993; 19:117
[10]Zik O,Moses E.Phys Rev,1996;53E:1760
[11]Shang C H.Phys Rev,1996;53B:13 759
[12]Samid-Merzel N,Lipson S,Tannhauser D.Physica,1998; 257A:413
[13]Yao W J,Wei B.J Alloys Compd,2004;366:165
[14]Wang C P,Liu X J,Ohnuma I,Kainuma R,Ishida K. Science,2002;297:990
[15]Smithells C J.Smithelles Metals Reference Book (Vol.8). 6th ed,London:Butterworths,1983:1
[16]Brener E,Muller-Krumbhaar H,Temkin D.Physica, 1998;249A:73
[17]Brener E,Muller-Krumbhaar H,Saito Y,Temkin D.Phys Rev,1993;47E:1151
[18]Ihle T,Muller-Krumbhaar H.Phys Rev Lett,1993;70: 3083
[19]Utter B,Bodenschatz E.Phys Rev,2005;72E:011601
[20]Anne R,Kopf-Sill,Homsy G M.Phys Fluids,1998;31
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!