| “SEAWEED”MORPHOLOGY IN Fe--Sn--Si TERNARY MONOTECTIC ALLOY |
| REN Lina; CAI E; FENG Sheng |
| Northwest Institute for Non--Ferrous Metal Research |
|
Cite this article:
REN Lina; CAI E; FENG Sheng. “SEAWEED”MORPHOLOGY IN Fe--Sn--Si TERNARY MONOTECTIC ALLOY. Acta Metall Sin, 2008, 44(3): 307-313 .
[1]Creuze J,Bertheer F,Tetor R,Legrand B.Phys Rev Lett, 2001;86:5735 [2]Wang N,Wei B.Mater Sci Eng,2003;A345:145 [3]Blum B,Hammer L,Schmidt Ch,Schmidt C,Meier W, Wieckhorst O,Muller S,Heinz K.Phys Rev Lett,2002; 89:266102 [4]Creuze J,Berthier F,Tetot R Legrand B.Phys Rev Lett, 2001;86:5735 [5]Akamatsu S,Faivre G,Ihle T.Phys Rev,1995;5E:4751 [6]Utter B,Ragnarsson R,Bodenschatz E.Phys Rev Lett, 2001;86:4604 [7]Ihle T,Muller-Krumbhaar H.Phys Rev Lett,1993;70: 3083 [8]McCloud K,Maher J.Phys Rep,1995;260:139 [9]Matsuyama T,Matsushita M.Crit Rev Microbiol,1993; 19:117 [10]Zik O,Moses E.Phys Rev,1996;53E:1760 [11]Shang C H.Phys Rev,1996;53B:13 759 [12]Samid-Merzel N,Lipson S,Tannhauser D.Physica,1998; 257A:413 [13]Yao W J,Wei B.J Alloys Compd,2004;366:165 [14]Wang C P,Liu X J,Ohnuma I,Kainuma R,Ishida K. Science,2002;297:990 [15]Smithells C J.Smithelles Metals Reference Book (Vol.8). 6th ed,London:Butterworths,1983:1 [16]Brener E,Muller-Krumbhaar H,Temkin D.Physica, 1998;249A:73 [17]Brener E,Muller-Krumbhaar H,Saito Y,Temkin D.Phys Rev,1993;47E:1151 [18]Ihle T,Muller-Krumbhaar H.Phys Rev Lett,1993;70: 3083 [19]Utter B,Bodenschatz E.Phys Rev,2005;72E:011601 [20]Anne R,Kopf-Sill,Homsy G M.Phys Fluids,1998;31 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|