| A study of intragranular slip and grain boundary sliding in fcc Pd |
|
Cite this article:
. A study of intragranular slip and grain boundary sliding in fcc Pd. Acta Metall Sin, 2008, 44(3): 257-262 .
|
|
|
|
|
Received: 23 November 2007
|
|
|
[1]Schiotz J,Di Tolla F D,Jacobsen K W.Nature,1998; 391:561 [2]Schiotz J,Jacobsen K W.Science,2003;301:1357 [3]Van Swygenhoven H.Phys Rev,2001;64B:224105 [4]Yamakov V,Wolf D,Phillpot S R,Mukherjee A K,Gleiter H.Natur Mater,2004;3:43 [5]Zelin M G,Mukherjee A K.Acta Mater,1995;43:2359 [6]Van Swygenhoven H,Derlet P M,Froseth A G.Nat Mater, 2004;3:399 [7]Froseth A G,Van Swygenhoven H,Derlet P M.Acta Mater,2004;52:2259 [8]Van Swygenhoven H,Derlet P M,Hasnaoui A.Phys Rev, 2002;66B:024101 [9]Van Swygenhoven H.Science,2002;296:66 [10]Chen M,Ma E,Hemker K J,Sheng H,Wang Y,Cheng X.Science,2003;300:1275 [11]Lu L,Shen Y,Chen X,Qian L,Lu K.Science,2004;304: 422 [12]Wang Y C,Li J H,Ye H Q.Philos Mag,1996;73A:213 [13]Foiles S M,Baskes M I,Daw M S.Phys Rev,1986;33B: 7983 [14]Wang Y C,Ye H Q.Philos Mag,1997;75A:261 [15]Sutton A P,Vitek V.Philos Trans R Soc,1983;309A:1 [16]Pond R C,Vitek V.Proc R Soc London,1977;357A:453 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|