Abstract Investigation of the local structure evolution and the glass formation in the Pd55Ni45 alloy melt rapidly cooled under high pressures is performed using molecular-dynamics simulations. The critical cooling rates for glass formation are reduced apparently with the pressure. With the increase of pressures, a more compacted local structure with more ideal icosahedra than defected icosahedra is obtained, which may possibly be one of the main factors for the contribution of the high pressure to the glass formation.
|
Received: 31 July 2007
|
[1]Li M,Johnson W L.Phys Rev Left,1993;70:1120 [2]Inoue A.Acta Mater,2000;48:279 [3]Johnson W L.MRS Bull,1999;24:42 [4]Johnson W L.Mater Sci Forum,1996;35:225 [5]Wang D,Li Y,Sun B B,Sui M L,Lu K,Ma E.Appl Phys Lett,2004;84:4029 [6]Tang M B,Zhao D Q,Pan M X,Wang W H.Chin Phys Lett,2004;21:901 [7]Duan G,Xu D,Zhang Q,Zhang G,Cagin T,Johnson W L,Goddard W A.Phys Rev,2005;71B:223208 [8]Xia L,Li W H,Fang S S,Wei B C,Dong Y D,J Appl Phys,2000;699:026103; Yao K F,Ruan F.Chin Phys Lett,2005;22:1481; Yao K F,Ruan F,Yang Y Q,Chen N.Appl Phys Lett, 2006;88:122106 [9]Zhang J Z,Zhao Y S.Nature,2004;430:332 [10]Zhang J Z,Zhao Y S.Nature,2005;437:1057 [11]Wang Y,Fang Y Z,Kikegawa T,Lathe C,Saksl K,Franz H,Schneider J R,Genward L,Wu F M,Liu J F,Jiang J Z.Phys Rev Lett,2005;95:155501 [12]Steinhardt P J,Nelson D R,Ronchetti M.Phys Rev,1993; 28B:784 [13]Nakano H,Qi D W,Wang S.J Chem Phys,1989;90:1871 [14]Qi D W,Wang S.J Non-Cryst Solid,1991;13:573 [15]Coluzzi B,Parisi G,Verrocchio P.Phys Rev Lett,2000; 84:306 [16]Morishita T.Phys Rev Lett,2006;97:165502 [17]Li H,Pederiva F.Phys Rev,2005;71B:054513 [18]Shen Z Y,Chen G Y,Zhang Y,Yin X J.Phys Rev,1989; 39B:2714 [19]Wang W K,Iwasaki H,Fukamichi K.J Mater Sci,1980; 15:2701 [20]K(?)ga J,Okumura H,Nishio K,Yamaguchi T,Yonezawa F.Phys Rev,2002;66B:064211 [21]Wang W H,Okada T,Wen P,Wang X L,Pan M X,Zhao D Q,Utsumi W.Phys Rev,2003;68B:184105 [22]Fraenkel W,Stern A.Z Anorg Chem,1927;166:161 [23]Foiles S M.Phys Rev,1985;32B:3409 [24]Lu J,Szpunar J A.Philos Mag,1997;75:1057 [25]Verlet V.Phys Rev,1967;159:98 [26]Andersen H C.J Chem Phys,1980;72:4 [27]Weaire D.J Phys,1968;C1:210 [28]Honeycutt J D,Andersen H C.J Phys Chem,1987;91: 4950 [29]Qi L,Zhang H F,Hu Z Q,Liaw P K.Phys Lett,2004; 327A:506 [30]Rahman A,Mandell M J,McTague J P.J Chem Phys, 1976;64:3215 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|