| THE OBSERVATION AND ANALYSIS OF ε-Cu PHASE IN THE CU CONTAINING ANTIBACTERIAL AUSTENITESTAINLESS STEEL |
| hengwu li;; |
| 上海天宝不锈钢有限公司 |
|
Cite this article:
hengwu li. THE OBSERVATION AND ANALYSIS OF ε-Cu PHASE IN THE CU CONTAINING ANTIBACTERIAL AUSTENITESTAINLESS STEEL. Acta Metall Sin, 2008, 44(1): 39-42 .
|
|
|
Abstract The paper presented Some results about ε-Cu phases formed during antibacterial treatment in the antibacterial stainless steel by LM,X-Ray, SEM,EPM and TEM, and then discussed form process ε-Cu phases.
|
|
Received: 10 April 2007
|
|
|
[1]Nakamura S,Ookubo N,Miyakusu K,Hasegawa M.Nis- shin Steel Technical Rep,1997;76:48 (中村定幸,大久保直人,宫楠克久,长谷川守弘.日新制钢技报,1997;76:48) [2]Ookubo N,Nakamura S,Yamamoto M,Miyakusu K, Hasegawa M.Nisshin Steel Technical Rep,1998;77:61 (大久保直人,中村定幸,山本正人,宫楠克久,长谷川守弘日新制钢技报,1998;77:61) [3]Yamamoto M.Spec Steels,1999;48(6):24 (山本正人.特殊钢,1999;48(6):24) [4]Yokota T,Tochihara M,Ohta M.Kawasaki Steel Technol Rep,2001;33:88 (横田毅,枥原美佐子,太田稚之.川崎制铁技报,2001;33:88) [5]Yang K,Chen S H,Dong J S,LüM Q.Met Funct Mater, 2005;12(6):6 (杨柯,陈四红,董加胜,吕曼祺.金属功能材料,2005;12(6):6) [6]Chen S H,LüM Q,Zhang J D,Dong J S,Yang K.Acta Metall Sin,2004;40:314 (陈四红,吕曼祺,张敬党,董加胜,杨柯.金属学报,2004;40:314 [7]LüM Q,Chen S H,Dong J S,Yang K.Met Funct Mater, 2005;12(6):10 (吕曼祺,陈四红,董加胜,杨柯.金属功能材料,2005;12(6):10) [8]Zhang T B,Zhang T Y.Chin Pat,ZL 02 1 48742.1,2007 (张体宝,张体勇.中国发明号利,ZL02148742.1,2007) [9]Zhou J,Chang X,Guo K X.Acta Metall Sin,1978;14: 246 (周敬,常昕,郭可信.金属学报,1978;14:246) [10]Zhou Y X,Huang Q Z,Chen Q T,Deng D Q,Pu S K. Acta Metall Sin,1978;14:292 (周永忻,黄清珠,陈乾惕,邓定庆,蒲绍康.金属学报,1978;14:292) [11]Thompson S W,Krauss G.Metall Mater Trans,1996; 27A:1573 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|