| EFFECT OF HOMOGENIZATION TREATMENT ON THE MICROSTRUCTURES OF LOW FREQUENCY ELECTROMAGNETIC CASTING 7050 ALUMINUM ALLOY |
| Zhihao Zhao;;; |
| 东北大学材料电磁过程教育部重点实验室 |
|
Cite this article:
Zhihao Zhao. EFFECT OF HOMOGENIZATION TREATMENT ON THE MICROSTRUCTURES OF LOW FREQUENCY ELECTROMAGNETIC CASTING 7050 ALUMINUM ALLOY. Acta Metall Sin, 2007, 43(9): 956-960 .
|
|
|
Abstract The 7050 aluminum alloy ingot with fine microstructure was cast by low frequency electromagnetic casting (LFEC) process. The homogenization treatment behaviors of LFEC ingot were investigated experimentally. The results show that the ingots cast with low frequency electromagnetic field has a better homogenization effect than conventional DC ingot. Under the same homogenization condition, the LFEC ingot has fewer low melting point phase between grains and more solute elements inside grains. After homogenized for 12 hours the LFEC ingots can reach the average percentage of the alloy elements, but the DC ingots haven’t reach it until for 48 hours.
|
|
Received: 10 January 2007
|
|
|
[1]Birat J P,Chone J.lronmaking Steelmaking,1983;110: 269 [2]Vires C,Ricou R.Metall Trans,1985;16B:377 [3]Meyer J L,Szekely J,Elkaddah N,Vires C,Ricou R.Met- all Trans,1987;18B:529 [4]Beitelman L.Can Metall Q,1999;38:301 [5]Spitzer K H,Reiter G,Schwerdtfeger K.ISIJ Int,1996; 36:487 [6]Vives C.Metall Trans,1989;20B:623 [7]Vives C.Metall Trans,1989;20B:631 [8]Dong J,Cui J Z.Metall Mater Trans,2004;35A:2487 [9]Zhang B J,Cui J Z,Lu G M,Zhang Q,Ban C Y.Acta Metall Sin,2002;38:215 (张北江,崔建忠,路贵民,张勤,班春燕.金属学报,2002;38:215) [10]Zhang B J,Cui J Z.Mater Sci Eng,2003;A355:325 [11]Zhao Z H,Wang J,Zuo Y B,Cui J Z.Acta Metall Sin, 2007;43:949 (赵志浩,王静,左玉波,崔建忠.金属学报,2007;43:949) [12]Chandan M,Mukhopadhyay A K.Mater Sci Eng,2005; A391:367 [13]Robson J D.Mater Sci Eng,2004;A382:112 [14]Desnain P,Fautrelle Y,Meyer J L,Riquet J P,Durand F. Acta Metall Mater,1988;38:1513 [15]Stefanescu D M,Padhya G,Yopdhyay D B.Metall Trans, 1990;21A:998 [16]Zhang B J,Cui J Z,Lu G M.Mater Lett,2003;57:1707 [17]Liu X T,Dong J,Cui J Z.Trans Nonferrous Met Soc Chin,2003;13:909 (刘晓涛,董杰,崔建忠.中国有色金属学报,2003;13:909) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|