Effect of the electromagnetic vibration on the distribution and morphology of primary silicon in Al-Si hypereutectic alloy solidified under a high magnetic field
YU Jian-Bo
上海大学
Cite this article: 

YU Jian-Bo. Effect of the electromagnetic vibration on the distribution and morphology of primary silicon in Al-Si hypereutectic alloy solidified under a high magnetic field. Acta Metall Sin, 2007, 43(9): 994-998 .

Download:  PDF(397KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of electromagnetic vibration on the distribution and morphology of primary silicon in the Al-18wt%Si alloy has been investigated systematically in this paper. The experimental results show that the primary silicon agglomerated and expelled to the top of the sample when the magnetic intensity is low(2T). The ssegregation of silicon grains decreased gradually and the phenomenon of agglomerating disappeared with the increase of magnetic intensity (10T), and the star-like coarse primary silicon turned refined flake or square. It is shown that the movement of primary silicon is depended on gravity and the effective viscous force caused by the magnetic field,and the terminal migration velocity is proportional to the radium of primary silicon and inversely to the intensity of magnetic field. The observed results are approximately agreed with the theoretical analysis.
Key words:       
Received:  10 January 2007     
ZTFLH:  TG111.4  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I9/994

[1]David P.Mod Cast,1990;82(2):55
[2]Pan E N,Hu J F.AFS Trans,1998;105:413
[3]Bunk W G.Mater Sci Eng,1991;A134:1087
[4]Vives C.Mater Sci Eng,1993;A173:169
[5]Vives C.J Cryst Growth,1996;158:118
[6]Radjai A,Miwa K,Nishio T.Metall Mater Trons,1998; 29A:1477
[7]Radjai A,Miwa K,Nishio T.Metall Mater Trans,2002; 33A:3025
[8]Takagi T,Iwai K,Asai S.ISIJ Int,2003;43:842
[9]Iwai K,Sugiura K.Mater Sci Forum,2005;475:2695
[10]Wang H L,Ren Z M,Ren W L,Wang J,Deng K,Zhong Y B.Shanghai Met,2006;28(5):40 (王洪亮,任忠鸣,任维丽,王俊,邓康,钟云波.上海金属,2006;28(5):40)
[11]Ren W L,Ren Z M,Wang H L,Zhong Y B,Deng K,Yu J B.Mater Sci Technol,in press (任维丽,任忠鸣,王洪亮,钟云波,邓康,余建波.材料科学与工艺,待发表)
[12]Wang J,Deng K,Ren Z M,Ren W L,Li X,Zhong Y B, Xu K D.Shanghai Met,2006;28(6):7 (王俊,邓康,任忠鸣,任维丽,李喜,钟云波,徐匡迪.上海金属,2006;28(6):7)
[13]Zhang Q,Cui J Z.Chin J Nouferrous Met,2003;13:1500 (张勤,崔建忠.中国有色金属学报,2003;13:1500)
[14]Mao W M,Li S S,Zhao A M,Cui C L,Zhong X Y.Mater Sci Technol,2001;9:117 (毛为民,李树索,赵爱民,崔成林,钟雪友.材料科学与工艺,2001;9:117)
[15]Zhang B W.PhD Dissertation,Shanghai University,2003: 26 (张邦文.上海大学博士学位论文,2003:26)
[16]Zhou Y H,Hu Z Q,Jie W Q.Solidification Technology. Beijing:China Machine Press,1998:46 (周尧和,胡壮麒,介万奇.凝固技术.北京:机械工业出版社,1998:46)7
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!