| Effect of the electromagnetic vibration on the distribution and morphology of primary silicon in Al-Si hypereutectic alloy solidified under a high magnetic field |
| YU Jian-Bo |
| 上海大学 |
|
Cite this article:
YU Jian-Bo. Effect of the electromagnetic vibration on the distribution and morphology of primary silicon in Al-Si hypereutectic alloy solidified under a high magnetic field. Acta Metall Sin, 2007, 43(9): 994-998 .
|
|
|
Abstract The effect of electromagnetic vibration on the distribution and morphology of primary silicon in the Al-18wt%Si alloy has been investigated systematically in this paper. The experimental results show that the primary silicon agglomerated and expelled to the top of the sample when the magnetic intensity is low(2T). The ssegregation of silicon grains decreased gradually and the phenomenon of agglomerating disappeared with the increase of magnetic intensity (10T), and the star-like coarse primary silicon turned refined flake or square. It is shown that the movement of primary silicon is depended on gravity and the effective viscous force caused by the magnetic field,and the terminal migration velocity is proportional to the radium of primary silicon and inversely to the intensity of magnetic field. The observed results are approximately agreed with the theoretical analysis.
|
|
Received: 10 January 2007
|
|
|
[1]David P.Mod Cast,1990;82(2):55 [2]Pan E N,Hu J F.AFS Trans,1998;105:413 [3]Bunk W G.Mater Sci Eng,1991;A134:1087 [4]Vives C.Mater Sci Eng,1993;A173:169 [5]Vives C.J Cryst Growth,1996;158:118 [6]Radjai A,Miwa K,Nishio T.Metall Mater Trons,1998; 29A:1477 [7]Radjai A,Miwa K,Nishio T.Metall Mater Trans,2002; 33A:3025 [8]Takagi T,Iwai K,Asai S.ISIJ Int,2003;43:842 [9]Iwai K,Sugiura K.Mater Sci Forum,2005;475:2695 [10]Wang H L,Ren Z M,Ren W L,Wang J,Deng K,Zhong Y B.Shanghai Met,2006;28(5):40 (王洪亮,任忠鸣,任维丽,王俊,邓康,钟云波.上海金属,2006;28(5):40) [11]Ren W L,Ren Z M,Wang H L,Zhong Y B,Deng K,Yu J B.Mater Sci Technol,in press (任维丽,任忠鸣,王洪亮,钟云波,邓康,余建波.材料科学与工艺,待发表) [12]Wang J,Deng K,Ren Z M,Ren W L,Li X,Zhong Y B, Xu K D.Shanghai Met,2006;28(6):7 (王俊,邓康,任忠鸣,任维丽,李喜,钟云波,徐匡迪.上海金属,2006;28(6):7) [13]Zhang Q,Cui J Z.Chin J Nouferrous Met,2003;13:1500 (张勤,崔建忠.中国有色金属学报,2003;13:1500) [14]Mao W M,Li S S,Zhao A M,Cui C L,Zhong X Y.Mater Sci Technol,2001;9:117 (毛为民,李树索,赵爱民,崔成林,钟雪友.材料科学与工艺,2001;9:117) [15]Zhang B W.PhD Dissertation,Shanghai University,2003: 26 (张邦文.上海大学博士学位论文,2003:26) [16]Zhou Y H,Hu Z Q,Jie W Q.Solidification Technology. Beijing:China Machine Press,1998:46 (周尧和,胡壮麒,介万奇.凝固技术.北京:机械工业出版社,1998:46)7 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|