| MICROSTRUCTURAL EVOLUTION OF Ti-47Al ALLOY DURING DIRECTIONAL SOLIDIFICATION BY SEEDING METHOD |
| ;;;; |
| 西北工业大学 |
|
Cite this article:
. MICROSTRUCTURAL EVOLUTION OF Ti-47Al ALLOY DURING DIRECTIONAL SOLIDIFICATION BY SEEDING METHOD. Acta Metall Sin, 2007, 43(9): 897-902 .
|
|
|
Abstract Microstructural selection during the directional solidification (DS) of Ti-47Al grown from a Ti-43Al-3Si seed was studied. The high-temperature hexagonal close packed α-phase in a cellular growth condition were correctly oriented so that the DS ingot with fully lamellar microstructure parallel to DS direction was successfully obtained at growth rate of 90mm/h. As the liquid composition closed to Ti-47Al, because of the variation of growth rates and the effect of solidification interface morphologies on solute segregation, βphase started to nucleated and grown in the interdendritic of α phase, lamellar microstructures inclined with angles of 45º to the growth direction were grown, thus successful seeding from the Ti-43Al-3Si seed was interrupted. Fine α dendritic in preferred crystallographic direction were obtained when the growth rate increased to 720mm/h.
|
|
Received: 22 December 2006
|
[1]Inui H,Kishida K,Kobayashi M,Shirai Y,Yamaguchi M. Philos Mag,1995;72A:1609 [2]Johnson D R,Masuda Y,Yamanak T,Inui H,Yamaguchi M.Metall Mater Trans,2000;31A:2463 [3]Muto S,Yamanaka T,Lee N H,Johnson D R,Inui H, Yamaguchi M.Adv Eng Mater,2001;3:391 [4]Lee N H,Johnson D R,Inui H,Oh M H,Wee D M,Ya- maguchi M.Intermetallics,2002;10:841 [5]Lee N H,Johnson D R,Inui H,Oh M H,Wee D M,Ya- maguchi M.Mater Sci Eng,2002;A329-331:19 [6]Johnson D R,Inui H,Muto S,Omiya Y,Yamanaka T. Acta Mater,2006;54:1077 [7]Yamaguchi M,Johnson D R,Lee H N,Inui H.Inter- metallics,2000;8:511 [8]Zheng X Q,Shen J,Ding H S,Chen R R,Xu X.Mater Rev,2005;19(3):118 (郑循强,沈军,丁宏升,陈瑞润,许雄.材料导报,2005;19(3):118) [9]Luo W Z,Shen J,Li Q L,Man W W,Zheng X Q,Liu L, Fu H Z.Acta Metall Sin,2006;42:1238 (罗文忠,沈军,李庆林,满伟伟.郑循强,刘林,傅恒志.金属学报,2006;42:1238) [10]Lapin J,Ondrus L.Kovove Mater,2002;40(3):161 [11]Fu H Z,Su Y Q,Guo J J,Xu D M.Acta Metall Sin,2002; 38:1127 (傅恒志,苏彦庆,郭景杰,徐达鸣.金属学报,2002;38:1127) [12]Kim M C,Oh M H,Lee J H,Inui H,Yamaguchi M,Wee D M.Mater Sci Eng,1997;A239-240:570 [13]Jung I S,Kim M C,Lee J H,Oh M H,Wee D M.Inter- metallics,1999;7:1247 [14]Hunziker O,Vandyoussefi M,Kurz W.Acta Mater,1998; 46:6325 [15]Li S M,Liu L,Li X L,Fu H Z.Acta Metall Sin,2004;40: 20 (李双明,刘林,李晓历,傅恒志.金属学报,2004;40:20) [16]Liu C,Su Y Q,Li X Z,Guo J J,Jia J,Fu H Z.Acta Metall Sin,2005;41:260 (刘畅,苏彦庆,李新中,郭景杰,贾均,傅恒志.金属学报,2005;41:260) [17]Li S M,Du W,Zhang J,Li J S,Liu L,Fu H Z.Acta Metall Sin,2002;38:1195 (李双明,杜炜,张军,李金山,刘林,傅恒志.金属学报,2002;38:1195) [18]Hu H Q.Solidification Principle of Metals.Beijing:China Machine Press,2000:112 (胡汉起.金属凝固原理.北京:机械工业出版社,2000:112) [19]Fu H Z,Guo J J,Su Y Q,Liu L,Xu D M,Li J S.Chin J Nonfeerous Met,2003;13:797 (傅恒志,郭景杰,苏彦庆,刘林,徐达鸣,李金山.中国有色金属学报,2003;13:797) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|