Abstract  The influence of Al2O3 on vanadium concentration in V-bearing steelmaking slag was stud ied. It was found that the prior precipitated phase of Ca2SiO4(S)contained V and P reacts with (Al2O3)to produce a new V- bearing mineral(Ca3(V,P)2O8•nCa2SiO4),and gehlenite(Ca2 Al2SiO7),when the melt slag modified by Al2O3 cooled down to1623K slowly.As the content of (Al2O3)increasing, Ca2SiO4 will vanished.Because(Al2O3)continue to react with Ca2SiO4 in the new V- bearing mineral,to produce gehlenite. the vanadium concertration in Ca3(V,P)2O8•nCa2SiO4 will increase.results also indicate that the phase of Ca3(V,P)2O8•nCa2SiO4 will be produce enormously and vanadium content in Ca3(V,P)2O8• nCa2SiO4 is high by method of control Al2O3 content in slag. This results provides a solid basic for the design of vanadium concentration mineral and increased the content of vanadium in the V-enriched mineral as much as possible.
Key words:       
Received:  29 September 2007     
ZTFLH:  TF141.6  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I5/603

[1]Sui Z T,Zhang P X.Acta Mater,1999;47:1337
[2]Li Y H,Lou T P,Sui Z T.Acta Metall Sin,1999;35:1130 (李玉海,娄太平,隋智通.金属学报,1999;35:1130)
[3]Ma J W,Sui Z T,Chen B C.Trans Nonferrous Met Soc Chin Eng,2000;10(4):23
[4]Sui Z T,Zhang P X.Acta Metall Sin,1997;33:943 (隋智通,张培新.金属学报,1997;33:943)
[5]Sui Z T.J Chin Rare Earth Soc Eng,1998;16:731
[6]Zhang P X,Sui Z T.J Chin Ceram Soc,1996;24:558 (张培新,隋智通.硅酸盐学报,1996;24:558)
[7]Lou T P,Li Y H,Li L S,Sui Z T.J Chin Ceram Soc, 2000;28:255 (娄太平,李玉海,李辽沙,隋智通.硅酸盐学报,2000;28:255)
[8]Li Y H,Lou T P,Sui Z T.Chin J nonferrous Met,2000; 10(5):1 (李玉海,娄太平,隋智通.中国有色金属学报,2000;10(5):1)
[9]Zhang L,Li G Q,Lou T P,Sui Z T.Acta Metall Sin,2002; 38:400 (张力,李光强,娄太平,隋智通.金属学报,2002;38:400)
[10]Yu L,Dong Y C,Ye G Z,Du S C.Ironmaking Steelmaking, 2007;34:131
[11]Dong Y C,Wu X R,Li L S.ISIJ Int,2005;45:1238
[12]Wu X R,Li L S,Dong Y C.ISIJ Int,2007;47:402
[13]Wu X R,Li L S,Dong Y C.J Wuhan Univ Technol (Mater Sci),2005;20(2):63
[14]Yu L,Li L S,Dong Y C,Du S C.Metall Mater Trans, 2006;34B:1097
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!