Abstract The influence of Al2O3 on vanadium concentration in V-bearing steelmaking slag was stud
ied. It was found that the prior precipitated phase of Ca2SiO4(S)contained V and P reacts with (Al2O3)to produce a new V- bearing mineral(Ca3(V,P)2O8•nCa2SiO4),and gehlenite(Ca2 Al2SiO7),when the melt slag modified by Al2O3 cooled down to1623K slowly.As the content of (Al2O3)increasing, Ca2SiO4 will vanished.Because(Al2O3)continue to react with Ca2SiO4 in the new V- bearing mineral,to produce gehlenite. the vanadium concertration in Ca3(V,P)2O8•nCa2SiO4 will increase.results also indicate that the phase of Ca3(V,P)2O8•nCa2SiO4 will be produce enormously and vanadium content in Ca3(V,P)2O8•
nCa2SiO4 is high by method of control Al2O3 content in slag. This results provides a solid basic for the design of vanadium concentration mineral and increased the content of vanadium in the V-enriched mineral as much as possible.
|
|
Received: 29 September 2007
|
|
|
[1]Sui Z T,Zhang P X.Acta Mater,1999;47:1337 [2]Li Y H,Lou T P,Sui Z T.Acta Metall Sin,1999;35:1130 (李玉海,娄太平,隋智通.金属学报,1999;35:1130) [3]Ma J W,Sui Z T,Chen B C.Trans Nonferrous Met Soc Chin Eng,2000;10(4):23 [4]Sui Z T,Zhang P X.Acta Metall Sin,1997;33:943 (隋智通,张培新.金属学报,1997;33:943) [5]Sui Z T.J Chin Rare Earth Soc Eng,1998;16:731 [6]Zhang P X,Sui Z T.J Chin Ceram Soc,1996;24:558 (张培新,隋智通.硅酸盐学报,1996;24:558) [7]Lou T P,Li Y H,Li L S,Sui Z T.J Chin Ceram Soc, 2000;28:255 (娄太平,李玉海,李辽沙,隋智通.硅酸盐学报,2000;28:255) [8]Li Y H,Lou T P,Sui Z T.Chin J nonferrous Met,2000; 10(5):1 (李玉海,娄太平,隋智通.中国有色金属学报,2000;10(5):1) [9]Zhang L,Li G Q,Lou T P,Sui Z T.Acta Metall Sin,2002; 38:400 (张力,李光强,娄太平,隋智通.金属学报,2002;38:400) [10]Yu L,Dong Y C,Ye G Z,Du S C.Ironmaking Steelmaking, 2007;34:131 [11]Dong Y C,Wu X R,Li L S.ISIJ Int,2005;45:1238 [12]Wu X R,Li L S,Dong Y C.ISIJ Int,2007;47:402 [13]Wu X R,Li L S,Dong Y C.J Wuhan Univ Technol (Mater Sci),2005;20(2):63 [14]Yu L,Li L S,Dong Y C,Du S C.Metall Mater Trans, 2006;34B:1097 |