| Dynamic Transformation of Undercooling Austenite and Microstructure Refinement in a Eutectoid Steel |
| HUANG Qingsong; LI Longfei; YANG Wangyue;SUN Zuqing |
| The State Key Laboratory for Advanced Metals and Materials; University of Science and Technology Beijing |
|
Cite this article:
HUANG Qingsong; LI Longfei; YANG Wangyue; SUN Zuqing. Dynamic Transformation of Undercooling Austenite and Microstructure Refinement in a Eutectoid Steel. Acta Metall Sin, 2007, 43(7): 724-730 .
|
|
|
|
|
Received: 21 September 2006
|
|
|
[1]Ma E.Scr Mater,2003;49:663 [2]Langford G.Metall Trans,1977;8A:861 [3]Nam W J,Bae C M.Mater Sci Eng,1995;A203:278 [4]Hono K,Ohnuma M,Murayama M,Nishida S,Yoshie A. Scr Mater,2001;44:977 [5]Ivanisenko Y,Lojkowski W,Valiev R Z,Fecht H J.Acta Mater,2003;51:5555 [6]Robbins J L,Shepard O C,Sherby O D.J Iron Steel Inst London,1964;202:804 [7]Valiev R Z,Islamgaliev R K,AlexandrovⅣ.Prog Mater Sci,2000;45:103 [8]Furuhara T,Mizoguchi T,Maki T.ISIJ Int,2005;45:392 [9]Storojeva L,Ponge D,Kaspar R,Rabbe D.Acts Mater, 2004;52:2209 [I0]Languillaume J,Kapelski G,Baudelet B.Acts Mater, 1997;45:1201 [11]Qi J J,Yang W Y,Sun Z Q.J Univ Sci Technol Beijing, 2002;24:97 (齐俊杰,杨(?)玥,孙祖庆.北京科技大学学报,2002;24: 97) [12]Yang W Y,Hu A M,Qi J J,Sun Z Q.Chin J Mater Res, 2001;15:171 (杨(?)玥,胡安民,齐俊杰,孙祖庆.材料研究学报,2001; 15:171) [13]Yang W Y,Qi J J,Sun Z Q,Yang P.Acts Metall Sin, 2004;40:135 (杨(?)玥.齐俊杰,孙祖庆,杨平.金属学报,2004;40: 135) [14]Chen G A,Yang W Y,Sun Z Q.Acts Metall Sin,2007; 43:27 (陈国安,杨(?)玥,孙祖庆.金属学报,2007;43:27) [15]Guo Z H.Trans Mater Heat Treat,2003;24:1 (郭正洪.材料热处理学报,2003;24:1) [16]Hillert M.Decomposition of Austenite by Diffusional Pro- cesses.NewYork-London:Interscience Publishers,1962: 197 [17]Offerman S E,van Wildren L J G W,Van Dijk N H,Si- etsma J,Rekveldt M Th,Van der Zwaag S.Aeta Mater, 2003;51:927 [18]Wilde J,Cerezo A,Smith G D W.Scr Mater,2000;43: 39 [19]Gavriljuk V G.Mater Sci Eng,2003;A345:81 [20]Shin DH,Kim Y S,Lavernia E J.Acts Mater,2001;49: 2391 [21]Nam W J,Bae C M,Oh S J,Kwon S J.Set Mater,2000; 42:457 [22]Watte P,Van Humbeek J,Aernoudt E,Lefever I.Scr Mater,1996;34:89 [23]Toribio J,Ovejero E.Set Mater,1998;39:323 [24]Li J H,Shi Y F,Gao H W.Steel Material Metallograph. Shanghai:Shanghai Science and Technology Press,1981: 344 (李炯辉,施友方,高汗文.钢铁材料金相图谱.上海:上海科学技术出版社,1981:344) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|