| Thermodynamics Properties of Ternary Bath of Coloring Hot--Dip Galvanization |
| LE Qichi; CUI Jianzhong |
| Key Lab of Electromagnetic Processing of Materials; Ministry of Education; Northeastern University; Shenyang 110004 |
|
Cite this article:
LE Qichi; CUI Jianzhong. Thermodynamics Properties of Ternary Bath of Coloring Hot--Dip Galvanization. Acta Metall Sin, 2006, 42(11): 1182-1186 .
|
|
|
Abstract The activities and activity interaction parameters of two kinds of ternary alloy baths, Zn-Mn-Me and Zn-Ti-Me, were calculated by use of Shuanglin Chen model and Zhongting Ma expression. The results indicate that the activity of color generation element Mn or Ti increased as addition of Ni or Cu, where the effect of Ni is superior to Cu, however, the addition of Ti decreased the activity of Mn in Zn-Mn bath, and the opposite behavior for Mn in Zn-Ti. There is an inevitable relationship between the activity of components and color generation effectiveness. That is to say, the additives which can increase the activities of color generation elements would be in favor of improving the combination properties of hot-dip bath, and finally of color generation effectiveness. Therefore, Mn, Ni, and Cu are favorable elements for coloring hot-dip bath, and the advantages and disadvantages of Ti are related with its concentration, which is consistent with the results of technology experiments.
|
|
Received: 18 May 2006
|
|
|
[1] Cominco Ltd. UK Pat, GB 1 195 904, 1970 [2] Symth R W. US 3 530 013, 1970 [3] Symth R W. US 3 630 792, 1971 [4] Le Q C, Cui J Z. Acta Metall Sin (Engl Lett), 1999; 12: 1217 [5] Le Q C, Cui J Z. Mater Rev, 1999; 13(3): 63 (乐启炽,崔建忠.材料导报, 1999;13(3):63) [6] Le Q C, Cui J Z. Chin J Nonferrous Met, 1998; 8(Suppl.2): 98 (乐启炽,崔建忠.中国有色金属学报,1998;8(Suppl.2):98) [7] Le Q C, Cui J Z. Chin J Nonferrous Met, 2000; 10: 388 (乐启炽,崔建忠.中国有色金属学报, 2000;10:388) [8] Lu G M, Le Q C, Cui J Z. Chin J Nonferrous Met, 2002; 11: 95 (路贵民,乐启炽,崔建忠.中国有色金属学报,2001,11:95) [9] Miedema A R, de Chatel P F, de Boer F R. Physica, 1980; 100B: 1 [10] Tanaka T, Gokcen N A, Morita Z. Z Metallkd, 1990; 81: 349 [11] Le Q C, Zhang X J, Cui J Z, Lu G M. Acta Metall Sin, 2003; 39: 35 (乐启炽,张新建,崔建忠,路贵民.金属学报,2003;39:35) [12] Ding X Y, Wang W Z. Acta Metall Sin, 1994; 30: B444 (丁学勇,王文忠.金属学报,1994;30:B444) [13] Ding X Y, Fan P, Han Q Y. Acta Metall Sin, 1994; 30: B49 (丁学勇,范鹏,韩其勇.金属学报,1994;30:B49) [14] Toop G W. TMS-AIME, 1965; 233: 850 [15] Shen J Y, Hao Y W, Zhou C H, Ling L. Acta Metall Sin, 1996; 32: 943 (沈剑韵,郝耀武,周传华,凌铃.金属学报,1996;32:943) [16] Chen S L, Cui J Q, Chen T K, Zhou G Z. CALPHAD, 1989; 13: 225 [17] Zhang S B, Li D Z. Phase Diagram-Principle, Calculation and Application in Metallurgy. Beijing: Metallurgical Industry Press, 1986: 446 (张圣弼,李道子.相图-原理、计算及在冶金中的应用.北京:冶金工业出版社, 1986:446) [18] Wagner C. Thermodynamics of Alloys. Reading, Mass Addison-Wesley, 1962: 51 [19] Ma Z T, Ohser J, Janke D. Acta Metall Sin, 1998; 34: 753 (马中庭,Ohser J,Janke D.金属学报.1998;34:753) [20] Yu J Q, Yi W Z, Chen B D, Chen H J. Collection of Binary Alloy Phase Diagram. Shanghai: Shanghai Science and Technology Press, 1983: 585 (虞觉奇,易文质,陈邦迪,陈宏鉴.二元合金状态图集.上海科学技术出版社,1983:585) |