| Hydrogen Solubility in Pure Metals for Gasar Process |
| Hua-Wei ZHANG;; |
| 先进成形制造教育部重点实验室;清华大学机械工程系 |
|
Cite this article:
Hua-Wei ZHANG. Hydrogen Solubility in Pure Metals for Gasar Process. Acta Metall Sin, 2007, 43(2): 113-118 .
|
|
|
Abstract Many data on hydrogen solubility in pure metals usually used in Gasar process, such as Al, Mg, Cu, Ni and Fe, have been compiled. All data were transformed into the same form as lg[H]=-A/T+B+0.5*lg(PH2) , and good results for calculating solubility have been gained by averaging the values of solubility constant A and B respectively.
|
|
Received: 01 August 2006
|
|
|
[1]et al.Translated by Huang L Y,Yan M S.Gas in Non-ferrous Metals and Alloys.Beijing:Metallurgical Industry Press,1989:126,75,65,68(等著.黄良余,严名山译.有色金属及其合金中的气体.北京:冶金工业出版社,1989:126,75,65,68) [2]Foundry Institute of Chinese Mechanical Engineering So-ciety.Foundry Handbook Vol.3 Non-ferrous Cast Alloys.Beijing:China Machine Press,1999:2,29(中国机械工程学会铸造专业学会.铸造手册,第3卷:铸造非铁合金.北京:机械工业出版社,1999:2,29) [3]Manchester F D.Phase Diagrams of Binary Hydrogen Alloys.Materials Park,Ohio:ASM International,2000:4,83,46 [4]Anyalebechi P N.Scr Metall Mater,1995;33:1209 [5]Dong R J.Principles of Cast Alloy Melting.Beijing:China Machine Press,1991:151(董若璟.铸造合金熔炼原理.北京:机械工业出版社,1991:151) [6]Lu W H,Li L S,Huang L Y.Cast Alloy & Melting.Beijing:China Machine Press,1996:303,306(陆文华,李隆盛,黄良余.铸造合金及其熔炼.北京:机械工业出版社,1996:303,306) [7]Talbot D E J,Anyalebechi P N.Mater Sci Technol J,1988;4:1 [8]Yin Z X.Light Met,2006;(1):53 (尹卓湘.轻金属,2006;(1):53) [9]Zhou J R.Questions and Answers about Melting and Casting of Aluminium Alloys.Beijing:Metallurgical Industry Press,1987:55(周家荣.铝合金熔铸问笞.北京:冶金工业出版社,1987:55) [10]Eichenauer W,Hattenbach K,Pebler A.Z Metallkd,1961;52:682 [11]Lin R Y,Hoch M.Metall Trans,1989;20A:1785 [12]Scully J R,Young G A Jr,Smith S W.Mater Sci Forum,2000;331-337:1583 [13]Ichimura M,Sasajima Y,Imabayashi M.Mater Trans,JIM,1991;32:1109 [14]Ichimura M,Katsuta H,Sasajima Y,Imabayashi M.J Phys Chem Solids,1988;49(10):1259 [15]Zhang C F,Gong J S,Huang X R,Wang K G.Purification & Modification of Liquid Metals.Shanghai:Shanghai Science and Technology Press,1989:60(张承甫,龚建森,黄杏蓉,王凯歌.液态金属的净化与变质.上海:上海科学技术出版社,1989:60) [16]Fromm E,Gebhardt E.Gase und Kohlenstoff in Metallen.(Gas and Carbon in Metals).Berlin:Springer-Verlag,1976 [17]Shapovalov V I,Semik A P,Timchenko A G.Russia Metallurgy.1993;(3):25 [18](?)vrelid E,Flφistand G B,Rosenqvist T,Bakke P,Engh T A.Scand J Metall,1998;27(3):133 [19]Nishimura C,Komaki M,Amano M.J Alloy Compds,1999;293(1):329 [20]Bakke P,Lauritzen J L,Engh T A,Oymo D.Light Metals.New Orlears,Louisiana,1991:1015 [21]Huang Y C,Watanabe T,Komatsu R.In:Saito T ed,Proc 4th Int Confn Vacuum Metall,Tokyo,Japan:The Iron and Steel Institute of Japan,1974:176 [22]San-Martin A,Manchester F D.Bull Alloy Phase Diagrams,1987;8(5):431 [23]Verbetsky V N,Mitrokhin S V.In:Lewis F A,Aladjem A eds,Diffusion and Defect Data,Part B:Solid State Phenomena,(Vol.73-75)Switzerland:Scitec Publications Ltd,2000:503 [24]Yamamura S,Shiota H,Murakami K.Mater Sci Eng,2001;A318:137 [25]Sokolov V M,Fedorenko I V.Int J Hydrogen Energy,1996;21:931 [26]Schenck H,Lange K W.Arch Eisenhüttenwes,1966;37:739 [27]Schürmann E,Sittard M,V(?)iker R.Z Metallkd,1987;78:457 [28]Brandes E A,Brook G B.Smithells Metals ReferenceBook.7th ed.,Boston:Butterworth-Heinemann Ltd,1992:12-5 [29]McLellan R B,Oates W A.Acta Metall,1973;21:181 [30]Staeford S W,McLellan R B.Acta Metall,1974;22:1463 [31]Robertson W M.Z Metallkd,1973;64:436 [32]Louthan M R,Donovan J A,Caskey G R.Acta Metall,1975;23:745 [33]Serdyuk N P,Trofimenko V V,Dukelskii Y M.Metally,1992;(5):201(1992;(5):201) [34]Lei Y Q.Chemicophysics of Casting Process.Beijing:New Times Press,1982:161(雷水泉.铸造过程物理化学.北京:新时代出版社,1982:161) [35]Svoboda J M et al.Zhu P Y etc.,trans.Gases in Cast Metals.Beijing:China Machine Press,1984:18(Svoboda J M等著.Zhu P Y等译.铸造金属中的气体北京:机械工业出版社,1984:18) [36]Shi L.Thermodynamics of Metals and Alloys.Beijing:China Machine Press,1992:166(石霖.合金热力学.北京:机械工业出版社,1992:166) [37]Frohberg M G,Anik S.Arch Eisenhüettenwesen,1984;55(2):45 [38]Da Silva J R G,McLellan R B.J Less-Common Met,1976;50(1):1 [39]Da Silva J R G,Stafford S W,McLellan R B.J Less Common Met,1976;49:407 [40]Kubaschewski O.Iron-Binary Phase Diagrams.Berlin:Springer-Verlag,1982:46 [41]Quick N R,Johnson H H.Acta Metall,1978;26:903 [42]Fujita F E.In:Oriani R A,Hirth J P,Smialowski M eds,Hydrogen Degradation of Ferrous Alloys,New Jersey:Noyes Publications,1985:1 [43]Zhang H W,Li Y X,Liu Y.Acta Metall Sin,2006;42:1165(张华伟,李言祥,刘源.金属学报,2006;42:1165) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|