| The super-long fatigue behavior of the as-extruded ZK60 magnesium alloy |
| Xu Dao-Kui;; |
|
Cite this article:
Xu Dao-Kui. The super-long fatigue behavior of the as-extruded ZK60 magnesium alloy. Acta Metall Sin, 2007, 43(2): 144-148 .
|
|
|
Abstract In the super-long fatigue life regime (106~109 cyc), the fatigue behavior of the as-extruded ZK60 Mg alloy was studied. The results revealed that a plateau existed in the regime of 5×106 ~ 108 cyc, whereas the fatigue strength gradually decreased in the regime of 108~109 cyc, and the fatigue strength corresponding to 109 cyc was 90±5MPa. SEM fracture observation indicated that the fatigue crack mostly initiated at the surface or subsurface for the samples failed in the regime of 5×106 ~108 cyc, and at the interior non-metallic inclusion for the samples failed between 108 and 109 cycles. According to the observation and determination of the region size of the crack initiation, the fatigue strength was estimated, and compared with the experimental result.
|
|
Received: 29 May 2006
|
|
|
[1]Chen Z H.Magnesium Alloy.Beijing:Chemical Industry Press,2004:448(陈振华编著.镁合金.北京;化学工业出版社,2004:448) [2]Mayer H,Papakyriacou M.Int J Fatigue,2003;25:245 [3]Zeng R C,Han E H,Ke W,Liu L,Xu Y B.Chin J Mater Res,2005;19:1(曾荣昌,韩恩厚,柯伟,刘路,徐永波.材料研究学报,2005;19:1) [4]Mayer H,Papakyrincou M,Stanzl-Tschegg S E,Tschegg E,Zettl B,Lipowsky H,Stich A.Mater Corros,1999;50:81 [5]Horstemeyer M F,Yang N,Gall K,Mcdowell D L,Fan J,MGullett P.Acta Mater,2004;52:1327 [6]Wang Q G,Apelian D,Griffith J R.Proc Materials Solutions 98,Rosemont,IL,USA,Materials Park,OH:ASM International,1998:217 [7]Tokaji K,Kamakura M.Int J Fatigue,2004;26:1217 [8]Xu D K,Liu L,Xu Y B,Han E H.J Alloy Compd,(In press) [9]Ogarrevic V V,Stephens R I.Annu Rev Mater Sci,1990;20:141 [10]Zhang J M,Yang Z G,Zhang J F,Li G Y,Li S X,Hui W J,Weng Y Q.Acta Metall Sin,2005;41:145(张继明,杨振国,张建锋,李广义,李守新,惠卫军,翁宇庆.金属学报,2005;41:145) [11]Liu Z,Zhang K,Zeng X Q.The Basic Theory and Applications of Mg Matrix Light Alloys.Beijing:China Machine Press,2002:17(刘正,张奎,曾小勤.镁基轻质合金理论基础及其应用.北京:机械工业出版社,2002:17) [12]Zhang J M,Yang Z G,Li S X,Li G Y,Hui W J,Weng Y Q.Acta Metall Sin,2006;42:259(张继明,杨振国,李守新,李广义,惠卫军,翁宇庆.金属学报,2006;42:259) [13]Murakami Y,Endo M.Proc Behavior Short Fatigue Cracks.London:EGF,Mech Eng Publ,1986:27m |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|